Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.65 - 3.15 g/cc | 2.65 - 3.15 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL® 1270 Conductive Elastomer Description: Material of choice for high-end commercial applications; superior performance, in non-corrosive environments; tear trim compression and injection molding. A low durometer hardness elast.. |
|||
Specific Gravity | 2.65 - 3.35 g/cc | 2.65 - 3.35 g/cc | |
Parker Chomerics CHO-BOND 1029 Conductive Adhesive CHO-BOND® 1029 is a highly conductive silicone adhesive, intended for bonding Chomerics’ conductive silicone EMI gaskets to electrically conductive substrates. It is a two-component, siliver-plate.. |
|||
Specific Gravity | 2.65 g/cc | 2.65 g/cc | |
Malvern Minerals Novacite® 1250 Untreated Lamellar Quartz Filler/Extender Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
Specific Gravity | 2.65 g/cc | 2.65 g/cc | |
Malvern Minerals Novacite® 200 Untreated Lamellar Quartz Filler/Extender Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
Specific Gravity | 2.65 g/cc | 2.65 g/cc | |
Malvern Minerals Novacite® 325 Untreated Lamellar Quartz Filler/Extender Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
Specific Gravity | 2.65 g/cc | 2.65 g/cc | |
Malvern Minerals Novacite® Daper Untreated Lamellar Quartz Filler/Extender Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
Specific Gravity | 2.65 g/cc | 2.65 g/cc | |
Malvern Minerals Novacite® L-207A Untreated Lamellar Quartz Filler/Extender Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
Specific Gravity | 2.65 g/cc | 2.65 g/cc | |
Malvern Minerals Novacite® L-337 Untreated Lamellar Quartz Filler/Extender Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
Specific Gravity | 2.65 g/cc | 2.65 g/cc | |
Malvern Minerals Novakup® 1250 Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Specific Gravity | 2.65 g/cc | 2.65 g/cc | |
Malvern Minerals Novakup® 200 Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Specific Gravity | 2.65 g/cc | 2.65 g/cc | |
Malvern Minerals Novakup® 325 Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Specific Gravity | 2.65 g/cc | 2.65 g/cc | |
Malvern Minerals Novakup® Daper Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Specific Gravity | 2.65 g/cc | 2.65 g/cc | |
Malvern Minerals Novakup® L-207A Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Specific Gravity | 2.65 g/cc | 2.65 g/cc | |
Malvern Minerals Novakup® L-337 Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Specific Gravity | 2.65 g/cc | 2.65 g/cc | Mixed |
Tra-Con Tra-Duct 2958 Snap Cure Conductive Silver Epoxy Adhesive TRA-DUCT 2958 is a two-part, smooth paste of specially refined and processed epoxy and silver components, recommended for electronic, microelectronic and die-attach bonding and sealing applications .. |
|||
Specific Gravity | 2.65 g/cc | 2.65 g/cc | Mixed |
Tra-Con Tra-Duct 2924 Conductive Silver Epoxy Adhesive TRA-DUCT 2924 is a two part electrically conductive composition developed for low shrinkage, low resistivity bonding applications where good electrical and physical properties over a wide temperatur.. |
|||
Specific Gravity | 2.65 g/cc | 2.65 g/cc | |
Epoxy Technology EPO-TEK® H35-175MPLV Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H35-175MPLV is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-el.. |
|||
Specific Gravity | 2.65 g/cc | 2.65 g/cc | |
Asahi Glass Fluon® PA3540LT 10% Carbon Fiber, 30% Bronze, PTFE Filled Compound Fluon®PTFE FC has improved creep and wear resistance. A wide range of fillers such as glass fiber, graphite, bronze, carbon fiber are available. Information provided by Asahi Glass Company, Inc. |