Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.06 g/cc | 2.06 g/cc | ASTM D792 |
Quadrant EPP Fluorosint® HPV Mica-filled PTFE (ASTM Product Data Sheet) |
|||
Specific Gravity | 2.06 g/cc | 2.06 g/cc | Part A |
Epoxy Technology EPO-TEK® 320NC Optically Opaque Epoxy Material Description: A two component, black-colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific.. |
|||
Specific Gravity | 2.06 - 2.10 g/cc | 2.06 - 2.10 g/cc | ASTM D792 |
Adamas Adalon® 118 PTFE, 23/2% Carbon/Graphite Filled Information provided by Adamas, HPM |
|||
Specific Gravity | 2.06 g/cc | 2.06 g/cc | |
Bulk Molding Compounds BMC 604 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 604 molding compound is a low-cost, mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose material wit.. |