Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.98 g/cc | 1.98 g/cc | ASTM D792 |
3M Dyneon™ THV 500A Fluorothermoplastic
(discontinued **) THV 500A is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of an agglomerate. As an agglomerate, it can be used for c.. |
|||
Specific Gravity | 1.98 g/cc | 1.98 g/cc | ASTM D792 |
PolyOne Edgetek® SF-40GF-25MN1/000 PPS (Polyphenylene Sulfide), 40% Glass Fiber and 25% Mineral Filled
(disco Information provided by PolyOne™ Corporation |
|||
Specific Gravity | 1.98 g/cc | 1.98 g/cc | ASTM D297 |
Greene Tweed CHEMRAZ® 584 Perfluoroelastomer Greene Tweed’s Chemraz® 584, a cream-colored perfluoroelastomer, is a specialty compound formulated to outlast the most demanding chemical process applications. Because of its outstanding o.. |
|||
Specific Gravity | 1.98 g/cc | 1.98 g/cc | ASTM 792 |
Multibase Multi-Flex® D 4210 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Noise DampingOzone Resistant Thermal Stability, GoodStiffness, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsInformation p.. |
|||
Specific Gravity | 1.98 g/cc | 1.98 g/cc | ASTM D297 |
Greene Tweed CHEMRAZ® 570 Perfluoroelastomer Chemraz® 570, recommended for a wide variety of semiconductor equipment wet processing applications where stringent seal reliability and contamination control is required, offers excellent perfor.. |
|||
Specific Gravity | 1.98 g/cc | 1.98 g/cc | |
Silberline Silvex® 115-20-D Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Specific Gravity | 1.98 g/cc | 1.98 g/cc | |
Silberline Silvex® 225-20-D Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Specific Gravity | 1.98 g/cc | 1.98 g/cc | |
Silberline Sparkle Silvex® 755-20-D Sparkle Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Specific Gravity | 1.98 g/cc | 1.98 g/cc | |
Silberline Sparkle Silvex® 760-20-D Sparkle Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Specific Gravity | 1.98 g/cc | 1.98 g/cc | |
Silberline Sparkle Silvex® 795-20-D Sparkle Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Specific Gravity | 1.98 g/cc | 1.98 g/cc | |
Silberline Sparkle Silvex® 885-20-D Sparkle Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Specific Gravity | 1.98 g/cc | 1.98 g/cc | |
Silberline Silvex® 545-20-D Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Specific Gravity | 1.98 g/cc | 1.98 g/cc | |
3M Dyneon™ PFE 60Z Perfluoroelastomer Dyneon™ PFE 60 Z is a technically advanced peroxide curable perfluoroelastomer, designed to meet the challenges of demanding sealing applications. It’s fully fluorinated back bone structure provid.. |
|||
Specific Gravity | 1.98 g/cc | 1.98 g/cc | ASTM D792 |
3M Dyneon™ THVP 2030GZ Fluorothermoplastic Granules THVP 2030GZ is a very flexible, transparent fluoroplastic composed of fluorinated monomers. It is ideal for applications that require the good temperature, chemical and flame resistance of a fluorop.. |
|||
Specific Gravity | 1.98 g/cc | 1.98 g/cc | Part B; TM R050-16 |
Resinlab® EP1200 Black Casting Resin Resinlab™ EP1200 Black is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility and a low CTE. It meets the re.. |
|||
Specific Gravity | 1.98 g/cc | 1.98 g/cc | |
BYK Cloisite® 30B Nanoclay Cloisite® 30B is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.
Information provided by Southern Clay ProductsSouthern Clay P.. |