Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.79 g/cc | 1.79 g/cc | |
Premix Premi-Glas® 8101 Glass Reinforced Polyester BMC Description: Premi-Glas® 8101 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits: Ex.. |
|||
Specific Gravity | 1.79 g/cc | 1.79 g/cc | ASTM D792 |
PolyOne Elastamax™ HTE 1109 Styrene Butadiene Block Copolymer (SBC) with Mineral Filler
(discontinued **) |
|||
Specific Gravity | 1.79 - 1.85 g/cc | 1.79 - 1.85 g/cc | ASTM D 792 |
Karina 18/268-RG-GE (CS) Gray Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.79 g/cc | 1.79 g/cc | |
Silberline Sparkle Silver® 3622 Sparkle Silver® 3622 is a coarse, regular purity, non-leafing aluminum pigment. It is characterized by high sparkle, white face color, deep flop and low opacity.Applications: Automotive; General .. |
|||
Specific Gravity | 1.79 g/cc | 1.79 g/cc | |
Silberline Sparkle Silver® 3624 Sparkle Silver® 3624 is a coarse, brilliant, regular purity, non-leafing aluminum pigment popular for solvent-based general industrial coatings. This pigment can be used with tints to produce a w.. |
|||
Specific Gravity | 1.79 g/cc | 1.79 g/cc | |
Silberline Tufflake® 3645 Tufflake® aluminum pigments are circulation-resistant, specifically designed to withstand mechanical forces and maintain their target appearance. They are primarily used in automotive coating app.. |
|||
Specific Gravity | 1.79 g/cc | 1.79 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® XI-4208 PA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.79 g/cc | 1.79 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® XI-4208 PA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.79 g/cc | 1.79 g/cc | |
Silberline Sparkle Silver® 3122-AR Sparkle Silver® 3122-AR is a coarse, non-leafing, acid stain resistant aluminum flake pigment. It is characterized by high sparkle, a white face color and deep flop. The main applications are hig.. |
|||
Specific Gravity | 1.79 g/cc | 1.79 g/cc | |
Silberline Tufflake® 3120-AR Tufflake® aluminum pigments are circulation-resistant, specifically designed to withstand mechanical forces and maintain their target appearance. They are primarily used in automotive coating app.. |
|||
Specific Gravity | 1.79 g/cc | 1.79 g/cc | |
Silberline Tufflake® 3145-AR Tufflake® aluminum pigments are circulation-resistant, specifically designed to withstand mechanical forces and maintain their target appearance. They are primarily used in automotive coating app.. |
|||
Specific Gravity | 1.79 g/cc | 1.79 g/cc | |
Silberline Tufflake® 3620 Tufflake® aluminum pigments are circulation-resistant, specifically designed to withstand mechanical forces and maintain their target appearance. They are primarily used in automotive coating app.. |
|||
Specific Gravity | 1.79 g/cc | 1.79 g/cc | |
Silberline Tufflake® 3650 Tufflake® aluminum pigments are circulation-resistant, specifically designed to withstand mechanical forces and maintain their target appearance. They are primarily used in automotive coating app.. |
|||
Specific Gravity | 1.79 g/cc | 1.79 g/cc | ASTM D792 |
DuPont Performance Polymers Rynite® FR543 NC010 PET Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm.. |
|||
Specific Gravity | 1.79 g/cc | 1.79 g/cc | |
Bulk Molding Compounds BMC 620X Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620X molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Specific Gravity | 1.79 - 1.99 g/cc | 1.79 - 1.99 g/cc | molded |
Bulk Molding Compounds BMC A50-XHS Bulk molding compound Description: BMC A50XHS is a high strength bulk molding compound. It can be supplied in bulk or extruded in preweighted slugs. Due to the excellent flow and controlled reactivity, BMC A50XHS i.. |
|||
Specific Gravity | 1.79 - 1.99 g/cc | 1.79 - 1.99 g/cc | molded |
Bulk Molding Compounds BMC A50-XHS-U Bulk molding compound Description: BMC A50-XHS-U is a high strength bulk molding compound with a UL F1 rating for outdoor exposure. This material was specifically designed for outdoor lighting and electrical applications.. |
|||
Specific Gravity | 1.79 g/cc | 1.79 g/cc | DIN 53 479 |
Hippe PVDF Better mechanical strength compared to other fluorinated polymers. Tough and hard. High-grade electrical feature. Good weathering stability. Physiologically safe. Not as good as fluorinated pol.. |