Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.953 - 0.959 g/cc @Temperature 25.0 °C |
0.953 - 0.959 g/cc @Temperature 77.0 °F |
ASTM D4052 |
PolyOne Synplast™ 901P-N Di (Nonyl, Decyl, Undecyl) Phthalate Linear phthalate esterInformation provided by PolyOne |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ISO 1183 |
Polimeri Europa Eraclene® BC 86 High Density Polyethylene - Blow Molding Eraclene BC 86 is a high density polyethylene resin (HDPE) with antioxidants, suitable for blow molding application. It is especially recommended for the production of containers up to 20 liters.Er.. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ISO 1183 |
Polimeri Europa Eraclene® MM 74 U High Density Polyethylene - Injection Molding Eraclene MM 74 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.This grade has a narrow molecular weight distribution. The polym.. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ISO 1183 |
Polimeri Europa Eraclene® MM 74 High Density Polyethylene - Injection Molding Eraclene MM 74 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MM 74 is characterized by a good balance between rigidity and impact.. |
|||
Specific Gravity | 0.953 - 0.956 g/cc | 0.953 - 0.956 g/cc | ASTM D1505 |
LG Chemical SEETEC PB270 HDPE Features: This high molecular weight, hexane copolymer is tailored for light-weight blow-molded containers that require: Good stiffness and Excellent processabilityAdditives: Anti-OxidantsApplicatio.. |
|||
Specific Gravity | <= 0.953 g/cc | <= 0.953 g/cc | Hydrometer; ASTM D1298 |
LG Chemical Methyl Acrylate Features: Low Color - Refining process are improved for produce the low color. Color is the main quality factor that influence the property of the final products. Low Acidity - Through the multistag.. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ASTM D792 |
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of.. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ASTM D792 |
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou.. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ASTM D792 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ASTM D792 |
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of.. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ASTM D792 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ASTM D792 |
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou.. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ASTM D1505 |
A. Schulman LP642 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 642 is a narrow molecular weight copolymer, high-density polyethylene combining high flow for thin wall articles with excellent toughness. ApplicationApplications of LP 642 include fo.. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ASTM D792 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ASTM D792 |
A. Schulman LP481 Molding Grade High-Density Polyethylene DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ASTM D792 |
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of.. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ASTM D792 |
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou.. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ASTM D1505 |
A. Schulman LP642 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 642 is a narrow molecular weight copolymer, high-density polyethylene combining high flow for thin wall articles with excellent toughness. ApplicationApplications of LP 642 include fo.. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ASTM D792 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ASTM D792 |
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of.. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ASTM D1505 |
A. Schulman LP642 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 642 is a narrow molecular weight copolymer, high-density polyethylene combining high flow for thin wall articles with excellent toughness. ApplicationApplications of LP 642 include fo.. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ASTM D792 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ASTM D1505 |
A. Schulman LP642 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 642 is a narrow molecular weight copolymer, high-density polyethylene combining high flow for thin wall articles with excellent toughness. ApplicationApplications of LP 642 include fo.. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ASTM D792 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ASTM D792 |
A. Schulman LP481 Molding Grade High-Density Polyethylene DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ASTM D1505 |
Chevron Phillips Marlex® HP076 High Density Polyethylene, Pipe Grade This hexene copolymer is tailored for pipe applications that require:Good melt strengthGood pipe stiffnessOutstanding ESCRTypical corrugated pipe applications for HP076 include:Culverts and storm se.. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ASTM D792 |
Entec Hypel® PEHD8/.953 HDPE Available in North America Features: Food Contact Acceptable and High DensityAgency Ratings: FDA 21 CFR 177.1520RoHS Compliant Form: Pellets Information provided by Entec |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ASTM D1505 |
A. Schulman LP642 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 642 is a narrow molecular weight copolymer, high-density polyethylene combining high flow for thin wall articles with excellent toughness. ApplicationApplications of LP 642 include fo.. |
|||
Specific Gravity | 0.953 g/cc | 0.953 g/cc | ASTM D792 |
A. Schulman LP481 Molding Grade High-Density Polyethylene DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman. |