Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.860 - 0.920 g/cc | 0.860 - 0.920 g/cc | ASTM D 792 |
Karina 360-06/858-IS-SD Blue PVC Compound Non toxic polyolefinic compound recommended for production of stopper sealant for beverage bottles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | 15°C; ASTM D4052 |
ExxonMobil 629 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | 15.6°C; ASTM D4052 |
ExxonMobil 832 Mobil DTE 800 Series Mobil DTE 832 and 846 are superior performance turbine oils designed for use in steam turbines, gas turbines and combined cycle gas turbine (CCGT) applications under the most severe operating condit.. |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | |
ExxonMobil Mobil Clean 5W-20 5000 Mobil Clean 5000 is formulated from high quality base stocks combined with modern performance additives, including an advanced detergent system to provide excellent engine cleanliness at oil drain i.. |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | |
ExxonMobil Mobil Clean 5W-30 Motor Oil Mobil Clean Motor Oil is formulated from quality base stocks combined with the most modern performance additives, including an advanced detergent system to provide excellent engine cleanliness. Thes.. |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | 15°C; ASTM D1298 |
ExxonMobil Teresstic GT 32 Teresstic GT is a high-quality turbine oil formulated to provide effective day-in and day-out performance of steam turbine and gas turbine electricity generators and mechanical drive systems. Teress.. |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | 15.6°C; ASTM D4052 |
ExxonMobil 320 Mobilgear SHC XMP Series Mobilgear SHC XMP Series supreme performance, fully synthetic industrial gear oils designed to provide optimum equipment protection and oil life even under extreme conditions. Mobil polyalphaolefin .. |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | 15°C; ASTM D4052 |
ExxonMobil 443 Mobilmet 440 Series Mobilmet 440 Series fluids are high performance, multi-service, non-corrosive straight cutting fluids. They are designed for moderate to heavy duty cutting operations. They are also suitable for m.. |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | ASTM D1298 |
ExxonMobil Mobilarma 777 The Mobilarma 700 Series contains three premium performance rust preventives that cover a range of applications including storage and inter-operational activities. The Mobilarma 777 and 778 are inte.. |
|||
Specific Gravity | 0.860 g/cc @Temperature 25.0 °C |
0.860 g/cc @Temperature 77.0 °F |
|
Dow Corning MOLYKOTE® PG-75 GREASE Semi-Synthetic (Mineral/PAO) grease especially for vehicle track-rod jointsInformation provided by Dow Corning |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | 15.6°C; ASTM D4052 |
ExxonMobil 320 Mobilgear SHC XMP Series Mobilgear SHC XMP Series supreme performance, fully synthetic industrial gear oils designed to provide optimum equipment protection and oil life even under extreme conditions. Mobil polyalphaolefin .. |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | 15°C; ASTM D4052 |
ExxonMobil 443 Mobilmet 440 Series Mobilmet 440 Series fluids are high performance, multi-service, non-corrosive straight cutting fluids. They are designed for moderate to heavy duty cutting operations. They are also suitable for m.. |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | 15°C; ASTM D4052 |
ExxonMobil 626 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | 15°C; ASTM D4052 |
ExxonMobil 629 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | 15.6°C; ASTM D4052 |
ExxonMobil 832 Mobil DTE 800 Series Mobil DTE 832 and 846 are superior performance turbine oils designed for use in steam turbines, gas turbines and combined cycle gas turbine (CCGT) applications under the most severe operating condit.. |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | |
ExxonMobil Mobil Clean 5W-20 5000 Mobil Clean 5000 is formulated from high quality base stocks combined with modern performance additives, including an advanced detergent system to provide excellent engine cleanliness at oil drain i.. |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | |
ExxonMobil Mobil Clean 5W-30 Motor Oil Mobil Clean Motor Oil is formulated from quality base stocks combined with the most modern performance additives, including an advanced detergent system to provide excellent engine cleanliness. Thes.. |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | ASTM D1298 |
ExxonMobil Mobilarma 777 The Mobilarma 700 Series contains three premium performance rust preventives that cover a range of applications including storage and inter-operational activities. The Mobilarma 777 and 778 are inte.. |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | 15°C; ASTM D1298 |
ExxonMobil Teresstic GT 32 Teresstic GT is a high-quality turbine oil formulated to provide effective day-in and day-out performance of steam turbine and gas turbine electricity generators and mechanical drive systems. Teress.. |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | 60°F; ASTM D-1298 |
ConocoPhillips ANDEROL® 6220 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | 60°F; ASTM D-1298 |
ConocoPhillips ANDEROL® 6320 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | ASTM D-1298 |
ConocoPhillips ANDEROL® HTC Chain & Way Fluid, Synthetic Food Grade ISO 220 Description: ANDEROL HTC Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the USDA where incidental fo.. |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | ASTM D-1298 |
ConocoPhillips ANDEROL® HTC Chain & Way Fluid, Synthetic Food Grade ISO 460 Description: ANDEROL HTC Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the USDA where incidental fo.. |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | |
Dow Corning Z-1224 TRIMETHYLCHLOROSILANE Information provided by Dow Corning |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | 15°C; ASTM D4052 |
ExxonMobil 627 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Specific Gravity | 0.860 g/cc @Temperature 25.0 °C |
0.860 g/cc @Temperature 77.0 °F |
|
Dow Corning 2502 Cosmetic Fluid A linear polydimethylsiloxane with randomly distributed alkyl chains for use in skincare, woundcare, haircare, suncare, and color cosmetic applications.Information provided by Dow Corning |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | |
ATG s.r.l. EPDM Ethylene-Propylene Terpolymer |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | ASTM D792 |
3D Systems CastForm™ PS Plastic for SLS® Systems For use with all selective laser sintering (SLS®) systems.ApplicationsCreate patterns directly rather than through indirect methodsComplex investment casting patternsReactive metals like titaniumLo.. |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | 60°F; ASTM D-1298 |
ConocoPhillips ANDEROL® 6150 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Specific Gravity | 0.860 g/cc | 0.860 g/cc | 15°C; ASTM D4052 |
ExxonMobil 626 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |