Polymer Property : Spiral Flow = 9.84 in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 25.0 - 76.0 cm
9.84 - 29.9 in
Average value: 58.5 cm Grade Count:13
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Spiral Flow 25.0 cm

@Thickness 2.50 mm
9.84 in

@Thickness 0.0984 in
at 254°C melt temp.
Covestro Bayblend® KU2-1500 Polycarbonate + ABS Blend, Extrusion/Blow-Molding  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Spiral Flow 25.0 - 25.0 cm

@Temperature 300 - 300 °C
9.84 - 9.84 in

@Temperature 572 - 572 °F
Average value: 25.0 cm Grade Count:1
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor..
Spiral Flow 25.0 cm

@Temperature 300 °C
9.84 in

@Temperature 572 °F
Solvay Method
Solvay Specialty Polymers Primef® 4002 40% GF PPS, High Fluidity Grade  (discontinued **)
Used for injection molding of high performance parts.