Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 61.0 cm | 24.0 in | |
PolyOne Geon™ Vinyl Rigid Molding M5015 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Spiral Flow | 61.0 cm | 24.0 in | |
PolyOne Geon™ Vinyl Rigid Molding M5200 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Spiral Flow | 61.0 cm | 24.0 in | |
PolyOne Geon™ Vinyl Rigid Molding M5240 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Spiral Flow | 61.0 cm | 24.0 in | |
PolyOne Geon™ Vinyl Rigid Molding M5240 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Spiral Flow | 61.0 cm @Thickness 2.50 mm |
24.0 in @Thickness 0.0984 in |
at 254°C melt temp. |
Covestro Bayblend® 2153 Polycarbonate + ABS Blend, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Spiral Flow | 61.0 cm @Thickness 2.50 mm |
24.0 in @Thickness 0.0984 in |
at 254°C melt temp. |
Covestro Bayblend® 2753 Polycarbonate + ABS Blend, Automotive
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Spiral Flow | 61.0 cm @Thickness 2.50 mm |
24.0 in @Thickness 0.0984 in |
at 254°C melt temp. |
Covestro Bayblend® T 45 Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy, good platable.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sep.. |
|||
Spiral Flow | 61.0 cm | 24.0 in | Cross Section: 7[mm]x3.5[mm]; AKRO |
Akro-Plastic Akromid® B3 GF 35 (2473) PA 6 Dry, 35% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Spiral Flow | 61.0 cm @Thickness 2.50 mm |
24.0 in @Thickness 0.0984 in |
at 254°C melt temp. |
Covestro Bayblend® FR 2010 Polycarbonate/ABS Blend
(discontinued **) Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Applications: Housings for office equipment, electrical engin.. |