Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 55.9 cm | 22.0 in | |
PolyOne Geon™ Vinyl Rigid Molding 6957 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Spiral Flow | 55.9 cm | 22.0 in | |
PolyOne Geon™ Vinyl Rigid Molding M5100 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Spiral Flow | 55.8 cm | 22.0 in | Exxon Method |
ExxonMobil Escorene® HD-6733 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: High Flow, Good StiffnessUses: Food containers, Small pails, Nursery containers |
|||
Spiral Flow | 56.0 cm @Temperature 220 °C |
22.0 in @Temperature 428 °F |
ASTM D3123 |
Total PS CPDS 863 High Flow Flame Retardant Deca Polystyrene Total Petrochemicals Polystyrene 863 is a high flow, heat resistant, high impact polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensiona.. |
|||
Spiral Flow | 56.0 cm | 22.0 in | MCI Method 1 |
Goodfellow TPX® MX002O Polymethylpentene This grade is highly recommended for injection molding, film and mandrel extrusion; also for fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefi.. |
|||
Spiral Flow | 56.0 cm @Thickness 2.50 mm |
22.0 in @Thickness 0.0984 in |
at 254°C melt temp. |
Covestro Bayblend® T 65 Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Interior automotive components.Information provided by Bayer.As of 1 September 2015,.. |