Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 45.5 cm | 17.9 in | Equistar |
LyondellBasell Microthene® MP574189 Linear Low Density Polyethylene, Injection Molding Grade ApplicationsMicrothene MP574189 exhibits excellent flow and impact with good stiffness. Typical applications include lids, closures, containers, housewares and medical items. MP574189 is 16 mesh pow.. |