Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 33.0 - 41.0 cm | 13.0 - 16.1 in | Average value: 36.3 cm Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Spiral Flow | 33.0 cm | 13.0 in | Exxon Method |
ExxonMobil Escorene® HD-6704 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Excellent Toughness, Excellent Stiffness, Excellent ESCRUses: Industrial containers, Industrial lids |
|||
Spiral Flow | 33.0 cm @Pressure 27.6 MPa, Temperature 163 °C |
13.0 in @Pressure 4000 psi, Temperature 325 °F |
Mesa |
Quantum Composites Lytex® 4149 55% Carbon Fiber Epoxy SMC Lytex 4149 is a high-performance, 3K tow carbon fiber (PAN) reinforced epoxy sheet molding compound designed for military and aerospace structural applications requiring excellent mechanical propert.. |
|||
Spiral Flow | 33.0 cm | 13.0 in | Measures the number on inches of flow produced when molten resin is injected into a long, spiral channel (0.625" insert), at a constant injection pressure of 1000 psi with a melt temperature of 440° F; Equistar |
LyondellBasell Alathon® H5618 High Density Polyethylene ApplicationsALATHON H 5618 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications inc.. |