Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.020 - 0.060 cm/cm @Thickness 3.18 mm |
0.020 - 0.060 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Edgetek® PS-30CF/000 HF UV BLACK Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.050 - 0.060 cm/cm @Thickness 3.20 mm |
0.050 - 0.060 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL MC4352 PP+Rubber+MF Description: Injection Molding, PP+Rubber+MF, Good Dimensional Stability, Scratch resistance, Good Weatherability, High ImpactApplication: Automotive Exterior (Sill Side Molding, Door Garnish)CAS: 9.. |