Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | Compression; ISO 2577 |
Raschig Group DECAL® 666/8 Phenolic Glass-fiber reinforced phenolic molding compound with mineral fillers. High heat resistance, reduced mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This prod.. |
|||
Linear Mold Shrinkage, Flow | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | Compression; ISO 2577 |
Raschig Group DECAL® 937 Phenolic Mica reinforced phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (W.. |
|||
Linear Mold Shrinkage, Flow | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | Injection and Compression; ISO 2577 |
Raschig Group EPOXIDUR® 3585 EP Epoxy, Molded, Glass Fiber Filler Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures, excel.. |
|||
Linear Mold Shrinkage, Flow | 0.00200 - 0.00500 cm/cm | 0.00200 - 0.00500 in/in | Injection; ISO 2577 |
Raschig Group RALUPOL® 802 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength, good heat resistance. This product meets the allowed up.. |
|||
Linear Mold Shrinkage, Flow | 0.00200 - 0.00500 cm/cm | 0.00200 - 0.00500 in/in | Injection; ISO 2577 |
Raschig Group RALUPOL® 804 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m.. |
|||
Linear Mold Shrinkage, Flow | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | Injection and Compression; ISO 2577 |
Raschig Group DECAL® 152CL Phenolic Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet.. |
|||
Linear Mold Shrinkage, Flow | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | Injection and Compression; ISO 2577 |
Raschig Group RESINOL® 400 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |