Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0081 - 0.0101 cm/cm

@Time 86400 sec
0.0081 - 0.0101 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP SH0430AC_BK1D466 PA12
4.3 specific gravity nylon 12, clean compound system
Linear Mold Shrinkage, Flow 0.0081 cm/cm
0.0081 in/in
ISO DIS 294-4
Wellman EcoLon® MRGF1518-BK3 38% Mineral/Glass Reinforced Post Consumer Compound Nylon 66
Description: Mineral/Glass Reinforced Post Consumer Compound Nylon 66Information provided by Wellman.