Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0075 - 0.0115 cm/cm | 0.0075 - 0.0115 in/in | |
LATI Latilub 88/10-10T Y/10 PEEK, 10% Aramid Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |