Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | Injection; ISO 2577 |
Raschig Group 2557 AMC Polyester Glass fiber reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, exceptional processability with short cycle time and low .. |
|||
Linear Mold Shrinkage, Flow | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | Compression; ISO 2577 |
Raschig Group DECAL® 572R Phenolic Glass-fiber reinforced phenolic molding compound. Exceptional heat resistance with regard to maintaining surface finish and mechanical properties, outstanding mechanical properties, excellent rotati.. |
|||
Linear Mold Shrinkage, Flow | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | Compression; ISO 2577 |
Raschig Group DECAL® 666/8 Phenolic Glass-fiber reinforced phenolic molding compound with mineral fillers. High heat resistance, reduced mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This prod.. |
|||
Linear Mold Shrinkage, Flow | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | Compression; ISO 2577 |
Raschig Group DECAL® 937 Phenolic Mica reinforced phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (W.. |
|||
Linear Mold Shrinkage, Flow | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | Injection and Compression; ISO 2577 |
Raschig Group EPOXIDUR® 3585 EP Epoxy, Molded, Glass Fiber Filler Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures, excel.. |
|||
Linear Mold Shrinkage, Flow | 0.00200 - 0.00500 cm/cm | 0.00200 - 0.00500 in/in | Injection; ISO 2577 |
Raschig Group RALUPOL® 4802 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |
|||
Linear Mold Shrinkage, Flow | 0.00200 - 0.00500 cm/cm | 0.00200 - 0.00500 in/in | Injection; ISO 2577 |
Raschig Group RALUPOL® 804 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m.. |
|||
Linear Mold Shrinkage, Flow | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | Injection and Compression; ISO 2577 |
Raschig Group RESINOL® 400 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |