Linear Mold Shrinkage, Flow 0.0105 - 0.014 cm/cm
0.0105 - 0.014 in/in
LATI Latamid 6 H-V0 PA 6, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good surface appearance.Availability: Africa & Middle East; Asi..
Linear Mold Shrinkage, Flow 0.0105 - 0.0135 cm/cm
0.0105 - 0.0135 in/in
LATI Latamid 66 H-V0 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
Linear Mold Shrinkage, Flow 0.0105 - 0.0135 cm/cm
0.0105 - 0.0135 in/in
LATI Latamid 6 BH PA 6, Heat Stabilized
Polyamide 6 (PA6). High fluidity. Heat stabilized. Very high fluidity.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter..
Linear Mold Shrinkage, Flow 0.0105 - 0.0135 cm/cm
0.0105 - 0.0135 in/in
LATI Latistat 62-08 PA6
Dissipative product based on Polyamide 6 (PA6). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S..
Linear Mold Shrinkage, Flow 0.0105 cm/cm
0.0105 in/in
BASF Procom® T20H S63 Polypropylene
Car heater casings.Data was collected by ISO methods and provided by BASF.
Linear Mold Shrinkage, Flow 0.0105 - 0.0135 cm/cm
0.0105 - 0.0135 in/in
LATI Latene® 9H TES/30 PP Homopolymer, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Aesthetic talc.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind..
Linear Mold Shrinkage, Flow 0.0105 - 0.0135 cm/cm
0.0105 - 0.0135 in/in
LATI Latimass 52/35-04 D009 PP Homopolymer
Specific density compound based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati..
Linear Mold Shrinkage, Flow 0.0105 - 0.013 cm/cm
0.0105 - 0.013 in/in
LATI Latilub 95-15T PSU, PTFE Filled
Self-lubricating product based on Polysulfone (PSU). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici ..