Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.00600 - 0.00800 cm/cm | 0.00600 - 0.00800 in/in | Injection; ISO 2577 |
Raschig Group DECAL® 1760 Phenolic Glass-fiber reinforced phenolic molding compound. Very good electrical properties, good chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals an.. |
|||
Linear Mold Shrinkage, Flow | 0.00600 - 0.00800 cm/cm | 0.00600 - 0.00800 in/in | Injection and Compression; ISO 2577 |
Raschig Group DECAL® 5431 Phenolic Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/.. |
|||
Linear Mold Shrinkage, Flow | 0.00600 cm/cm | 0.00600 in/in | Compression; ISO 2577 |
Raschig Group RALUPOL® 4566 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |