Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0049 cm/cm | 0.0049 in/in | ISO 294-4, 2577 |
Lanxess Pocan® B 4225 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding, flame retardant |
|||
Linear Mold Shrinkage, Flow | 0.0049 cm/cm @Time 86400 sec |
0.0049 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics NORYL WCP781 PPE-TPE Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto.. |
|||
Linear Mold Shrinkage, Flow | 0.0049 cm/cm @Time 86400 sec |
0.0049 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Asia Pacific) Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto.. |
|||
Linear Mold Shrinkage, Flow | 0.0049 cm/cm @Time 86400 sec |
0.0049 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Europe-Africa-Middle East) Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto.. |