Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0028 cm/cm
0.0028 in/in
ASTM D955
RheTech Products G20P100-00 20% Glass Fiber Reinforced Polypropylene, Natural
Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0028 cm/cm
0.0028 in/in
ASTM D955
RheTech Products G20P100-01 20% Glass Fiber Reinforced Polypropylene, Black
Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0028 cm/cm
0.0028 in/in
ASTM D955
RheTech Products G20P100-01UV 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, Black
Applications: Rigid exterior componentsHousingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0028 cm/cm
0.0028 in/in
ASTM D955
RheTech Products GC20P100-00 15% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0028 cm/cm
0.0028 in/in
ASTM D955
RheTech Products GC20P100-04 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, White
Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0028 cm/cm
0.0028 in/in
ASTM D955
RheTech Products GC20P100-177UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, (Chrysler HS5) Gray
Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0028 cm/cm
0.0028 in/in
ASTM D955
SK Chemicals SKYTHANE® 190A R series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Linear Mold Shrinkage 0.0028 cm/cm
0.0028 in/in
ASTM D955
SK Chemicals SKYTHANE® 195A R series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Linear Mold Shrinkage 0.0028 cm/cm
0.0028 in/in
ASTM D955
SK Chemicals SKYTHANE® R190A Polyether Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Linear Mold Shrinkage 0.0028 cm/cm
0.0028 in/in
ASTM D955
SK Chemicals SKYTHANE® R195A Polyether Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Linear Mold Shrinkage 0.0028 cm/cm
0.0028 in/in
320 x 320 mm flat plaque; ISO 1183
Azdel Plus C321B02N 32% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C321B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..
Linear Mold Shrinkage 0.0028 cm/cm
0.0028 in/in
ASTM D955
RheTech Products GC20P100-00UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Natural
Injection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0028 cm/cm
0.0028 in/in
ASTM D955
RheTech Products GC20P100-01 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0028 cm/cm
0.0028 in/in
ASTM D955
RheTech Products GC20P105-08FA 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, FDA Compliant, Black