Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.040 - 0.060 cm/cm | 0.040 - 0.060 in/in | |
Solvay Specialty Polymers Hyflon® PFA 450 Fluoropolymer
(discontinued **) Data provided by the manufacturer.Hyflon® PFA 450 has outstanding physical and chemical properties typical of fluoropolymers.Hyflon® PFA 420 |
|||
Linear Mold Shrinkage | 0.050 - 0.060 cm/cm | 0.050 - 0.060 in/in | ASTM D955 |
Lubrizol Isoplast® 300 Engineering Thermoplastic Polyurethane Resin Type: Isoplast® 300 is an engineering thermoplastic polyurethane resin.Appearance: Clear transparent pelletsApplication: Sheet extrusion, composite structures for industrial and consumer goods, inj.. |
|||
Linear Mold Shrinkage | 0.030 - 0.060 cm/cm | 0.030 - 0.060 in/in | |
Daikin NEOFLON NP-101 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: High speed wire and cable coatings.Information pro.. |
|||
Linear Mold Shrinkage | 0.030 - 0.060 cm/cm | 0.030 - 0.060 in/in | |
Daikin NEOFLON NP-120 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, cable jacketing, tubes.. |
|||
Linear Mold Shrinkage | 0.030 - 0.060 cm/cm | 0.030 - 0.060 in/in | |
Daikin NEOFLON NP-130 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Heavy wall wire insulation, cable jacketing, pipe, shrinka.. |
|||
Linear Mold Shrinkage | 0.030 - 0.060 cm/cm | 0.030 - 0.060 in/in | |
Daikin NEOFLON NP-21 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Suited to high speed extrusion .. |
|||
Linear Mold Shrinkage | 0.030 - 0.060 cm/cm | 0.030 - 0.060 in/in | |
Daikin NEOFLON NP-30 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, tubes, cable jacketing.. |
|||
Linear Mold Shrinkage | 0.030 - 0.060 cm/cm | 0.030 - 0.060 in/in | |
Daikin NEOFLON NP-40 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, transfer molding, compression molding.Applications: Films and s.. |
|||
Linear Mold Shrinkage | 0.030 - 0.060 cm/cm | 0.030 - 0.060 in/in | |
Daikin NEOFLON NP-20 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Wire and cable coatings, films,.. |
|||
Linear Mold Shrinkage | 0.030 - 0.060 cm/cm | 0.030 - 0.060 in/in | |
Daikin NEOFLON NP-3000 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Ultra high speed wire and cable coatings.Information provi.. |
|||
Linear Mold Shrinkage | 0.040 - 0.060 cm/cm | 0.040 - 0.060 in/in | |
Bulk Molding Compounds BMC SLC 2000 Glass Reinforced Polyester BMC SLC 2000 is a medium strength, low-cost, glass reinforced polyester compound with adjustable shrinkage. Ideal for circuit breakers, motor switch housings, fuse holders, brush holders, standoff i.. |