Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955-89 |
Multibase Multi-Pro® 0001 Black Polypropylene This product was specially designed for one customer's extrusion application needs. Data is taken from sample material only.Data provided by Multibase. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955 |
RheTech Products FT1004-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955 |
RheTech Products FT1004-625UV Thermoplastic Polyolefin, UV Stabilized, Interior DX9 Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955 |
RheTech Products HP514-01 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955 |
RheTech Products HP514-182 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 7701 Graphite Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955 |
RheTech Products HP514-197 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 848 Black Applications: Mirror housingsInterior trimCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955 |
RheTech Products HP514-199 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955 |
RheTech Products HP514-393 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 110D Medium Dark Pewter Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955 |
RheTech Products HP514-394 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 102E Medium Oak Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955 |
RheTech Products HP514-434 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9648 Medium Dark Neutral Applications: Interior trimCenter consolesFuse panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955 |
RheTech Products HP514-438 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 167 Ebony Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955 |
RheTech Products M15P100-01A 15% Mica Reinforced Polypropylene, Black Applications: Fan shroudsAir ductsElectronicsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | |
Plastcom SLOVAMID 66 T 40 FRO 3 PA66, 40% mineral filling, flame retardant FeaturesPA 66 with the content of 40% chemically modified mineral filling a with fire retardant. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat produ.. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | STN 64 0808 |
Plastcom SLOVAMID 66 T 40 Polyamide 66, 40% Mineral Filled FeaturesPA 66 with the content of 40% chemically modified mineral filling. Used for holders of electric hand tools, hobby tools, gears, covers of electric tools, flat products, automobile wheel cov.. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955 |
RheTech Products T20P250-00 20% Talc Reinforced Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Air ductsHush panelsWire troughBracketsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955 |
RheTech Products T20P250-01 20% Talc Reinforced Polypropylene Copolymer, Black Applications: Air ductsHush panelsWire troughBracketsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955 |
RheTech Products T20P250-699UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, AC20157-120 Black Applications: Window trimCowl screensExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955 |
RheTech Products T20P250-731UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, AS20698 Black Applications: Automotive trimIP componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955 |
RheTech Products T20P252-00 20% Talc Reinforced Polypropylene, Natural Applications: IP Structural componentsGlove box binWire troughInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955 |
RheTech Products T20P252-01 20% Talc Reinforced Polypropylene Copolymer, Black Applications: IP Structural componentsGlove box binWire troughInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955 |
RheTech Products T30P100-01 30% Talc Reinforced Polypropylene, Black Applications: BracketsAir ductsConsolesWire troughInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955 |
RheTech Products HP506-01A 21% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black Applications: Automotive interior applicationsHVAC ductsTail lamp housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955 |
RheTech Products HP514-00 14% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955 |
RheTech Products HP514-00UV 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Natural Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955 |
RheTech Products M12P256-01 12% Mica Reinforced Polypropylene Copolymer, Black Applications: Air damsAir ducts - distributionClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | |
Cytec EN-11 (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | |
Cytec EN-14 (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | |
Cytec EN-7 (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | |
Cytec EN-8 (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |
|||
Linear Mold Shrinkage | 0.0115 cm/cm | 0.0115 in/in | ASTM D955 |
PolyOne Synprene® RT-3615 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerNaturalApplications:General PurposeInteriorMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First ChoiceInformation.. |