Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0073 cm/cm
0.0073 in/in
Plastcom SLOVAMID 66 GF 33 PA66, 33% glass fibre
FeaturesChemically reinforced with 33% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. A..
Linear Mold Shrinkage 0.0073 cm/cm
0.0073 in/in
Isotropy
Solvay TECHNYL® A 218 V15 PA66, 15% glass fiber, DRY
Description: Polyamide 66, reinforced with 15% of glass fiber, heat stabilized, for injection molding.Available in: Latin AmericaProduct Applications: TECHNYL® A 218 V15 is used in all sectors of..
Linear Mold Shrinkage 0.0073 cm/cm
0.0073 in/in
Isotropy
Solvay TECHNYL® A 218W V15 PA66, 15% glass fiber, DRY
Description: Polyamide 66, reinforced with 15% of glass fiber, for injection molding, heat stabilized, with improved hydrolysis resistance.Available in: North AmericaProduct Applications: TECHNYL Â..
Linear Mold Shrinkage 0.0073 cm/cm
0.0073 in/in
Isotropy
Solvay TECHNYL® A 216 V15 Black 21N PA66, 15% glass fiber, DRY
Description: Polyamide PA66, reinforced with 15% of glass fiber, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 216 V15 is used in all sectors of industry, offer..
Linear Mold Shrinkage 0.0073 cm/cm
0.0073 in/in
ASTM D955
Plenco 4301 Phenolic, Granular, Injection Molded
PLENCO 04301 is a heat resistant, mineral filled phenolic molding compound offering excellent dimensional stability and electrical properties. UL recognized under component file E40654. 04301 is ava..