Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00600 cm/cm
0.00600 in/in
ASTM D955
Niche Polymer ABSN3BK ABS
Information provided by Niche Polymer
Linear Mold Shrinkage 0.00600 cm/cm
0.00600 in/in
ASTM D955
Niche Polymer ABSN4BK ABS
Information provided by Niche Polymer
Linear Mold Shrinkage 0.00600 cm/cm
0.00600 in/in
ASTM D955
Niche Polymer PA66GI14BK Nylon 66, 14% Glass Fiber Filled, Impact Modified
Information provided by Niche Polymer
Linear Mold Shrinkage 0.00600 cm/cm
0.00600 in/in
ASTM D955
Niche Polymer PCABSN10BK PC/ABS
Information provided by Niche Polymer
Linear Mold Shrinkage 0.00600 cm/cm
0.00600 in/in
ASTM D955
Niche Polymer PCABSN8BK PC/ABS
Information provided by Niche Polymer
Linear Mold Shrinkage 0.00600 cm/cm
0.00600 in/in
ASTM D955
Niche Polymer PCM12BK PC
Information provided by Niche Polymer
Linear Mold Shrinkage 0.00600 cm/cm
0.00600 in/in
ASTM D955
Niche Polymer PCM18BK PC
Information provided by Niche Polymer
Linear Mold Shrinkage 0.00600 cm/cm
0.00600 in/in
ASTM D955
Niche Polymer PCM6BK PC
Information provided by Niche Polymer
Linear Mold Shrinkage 0.00600 - 0.00900 cm/cm

@Temperature 80.0 - 121 °C
0.00600 - 0.00900 in/in

@Temperature 176 - 250 °F
Average value: 0.00750 cm/cm Grade Count:3
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v..
Linear Mold Shrinkage 0.00600 - 0.00900 cm/cm

@Time 3600 - 3600 sec
0.00600 - 0.00900 in/in

@Time 1.00 - 1.00 hour
Average value: 0.00750 cm/cm Grade Count:3
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v..
Linear Mold Shrinkage 0.00600 - 0.0212 cm/cm
0.00600 - 0.0212 in/in
Average value: 0.0113 cm/cm Grade Count:105
Overview of materials for Polypropylene with 30% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are..
Linear Mold Shrinkage 0.00600 - 0.0110 cm/cm
0.00600 - 0.0110 in/in
Average value: 0.00900 cm/cm Grade Count:5
Overview of materials for Nylon 12, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr..
Linear Mold Shrinkage 0.00600 - 0.0180 cm/cm
0.00600 - 0.0180 in/in
Average value: 0.0100 cm/cm Grade Count:9
Overview of materials for Ionomer, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma..
Linear Mold Shrinkage 0.00600 cm/cm
0.00600 in/in
Average value: 0.00600 cm/cm Grade Count:9
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend". Each property range of values reported is minimum and ma..
Linear Mold Shrinkage 0.00600 - 0.00900 cm/cm

@Temperature 80.0 - 121 °C
0.00600 - 0.00900 in/in

@Temperature 176 - 250 °F
Average value: 0.00750 cm/cm Grade Count:1
Overview of materials for Polypropylene with 10% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are ..
Linear Mold Shrinkage 0.00600 - 0.00900 cm/cm

@Time 3600 - 3600 sec
0.00600 - 0.00900 in/in

@Time 1.00 - 1.00 hour
Average value: 0.00750 cm/cm Grade Count:1
Overview of materials for Polypropylene with 10% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are ..
Linear Mold Shrinkage 0.00600 cm/cm
0.00600 in/in
Average value: 0.00600 cm/cm Grade Count:3
Overview of materials for ABS/Polyurethane Alloy
This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyurethane Alloy". Each property range of values reported is minimum and maximum values of appropr..