Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00300 cm/cm | 0.00300 in/in | ASTM D955 |
Niche Polymer PPHG30BK Homopolymer PP, 30% Glass Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00300 cm/cm | 0.00300 in/in | ASTM D955 |
Niche Polymer PPHG40BK Homopolymer PP, 40% Glass Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | Average value: 0.00400 cm/cm Grade Count:4 |
Overview of materials for Polyphthalamide (PPA), Stainless Fiber, EMI This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum va.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00600 cm/cm | 0.00300 - 0.00600 in/in | Average value: 0.00433 cm/cm Grade Count:3 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.0300 cm/cm | 0.00300 - 0.0300 in/in | Average value: 0.00981 cm/cm Grade Count:32 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.0180 cm/cm | 0.00300 - 0.0180 in/in | Average value: 0.0102 cm/cm Grade Count:24 |
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.0140 cm/cm | 0.00300 - 0.0140 in/in | Average value: 0.00582 cm/cm Grade Count:27 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00800 cm/cm | 0.00300 - 0.00800 in/in | Average value: 0.00450 cm/cm Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is m.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00850 cm/cm | 0.00300 - 0.00850 in/in | Average value: 0.00576 cm/cm Grade Count:7 |
Overview of materials for Phenolic, Novolac, Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron IPM2000 PMMA- ABS Alloy High Gloss, High scratch resistanceInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU602L ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU650N ABS Heat Resistant Medium/High ImpactInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU650NH ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron TG3MM ABS Injection Molding Grade Medium Flow, Medium Impact, high RigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron TG3MM ABS Injection Molding Grade Medium Flow, Medium Impact, high RigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU660 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU603 ABS Heat Resistant High Impact, High RigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU670M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00700 cm/cm | 0.00300 - 0.00700 in/in | Average value: 0.00518 cm/cm Grade Count:20 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.0400 cm/cm | 0.00300 - 0.0400 in/in | Average value: 0.0174 cm/cm Grade Count:39 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00800 cm/cm | 0.00300 - 0.00800 in/in | Average value: 0.00537 cm/cm Grade Count:18 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.0170 cm/cm | 0.00300 - 0.0170 in/in | Average value: 0.00566 cm/cm Grade Count:40 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU600N ABS Heat Resistant High ImpactInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU600N ABS Heat Resistant High ImpactInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00600 cm/cm | 0.00300 - 0.00600 in/in | Average value: 0.00450 cm/cm Grade Count:4 |
Overview of materials for Acrylic, Impact Modified Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified Sheet". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.0200 cm/cm | 0.00300 - 0.0200 in/in | Average value: 0.00955 cm/cm Grade Count:136 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00900 cm/cm | 0.00300 - 0.00900 in/in | Average value: 0.00600 cm/cm Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00800 cm/cm | 0.00300 - 0.00800 in/in | Average value: 0.00543 cm/cm Grade Count:7 |
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim.. |