Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | ASTM D955 |
RheTech Products F56-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Consumer goodsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | ASTM D955 |
RheTech Products FRG220-773UB 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Flame Retardant, UV Stabilized, Light Grey Applications: Electrical housingsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | ASTM D955 |
Oxford Polymers 40GF 40% Glass Fiber Reinforced Polyphenylene Sulfide 40% Glass Fiber Reinforced Polyphenylene SulfideInformation provided by Oxford Polymers. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0035 cm/cm | 0.0025 - 0.0035 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH GF5020 HC Polypropylene Homopolymer, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | Injection and Compression; ISO 2577 |
Raschig Group 2568 AMC Glass fiber-reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, heat resistant up to 500°C for short time - usable for s.. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | ASTM D955 |
RheTech Products F32-01 32% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Head lamp housingBracketsUnderhood componentsElectrical housingsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0035 cm/cm | 0.0025 - 0.0035 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH GF4030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | LATI |
LATI LASTANE 50 G/25 25% Glass Fiber Reinforced Polyurethane (PUR)
(Unverified Data**) Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0040 cm/cm | 0.0025 - 0.0040 in/in | ASTM D955 |
PolyOne Edgetek® ATH-20CF/000 Acetal-Homopolymer, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedElectrically ConductivePolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | (longitudinal); ISO 2577 |
Raschig Group 3572 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength and electrical strength, enhanced elasticity for ensuring good sealing under extreme heat and/or humidity, good chemical resis.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0030 cm/cm | 0.0025 - 0.0030 in/in | ASTM D955 |
PolyOne Lubri-Tech™ SF-25GF/13T-2S Polyphenylene Sulfide (PPS), Glass Filled, PTFE/Silicone Lubricated
(disco Description/Features:Glass Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | |
Haysite 54500 Polyester SMC, 35% Glass Reinforced A high strength fiberglass reinforced thermoset polyester compound formulated for injection, compression, or transfer molding. This material exhibits excellent electrical and mechanical properties, .. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0035 cm/cm | 0.0025 - 0.0035 in/in | |
Polyram PlusTek PA325G5 Nylon 6.6, 25% Glass Fiber, Flame Retardant 25% glass fiber reinforced, flame retardant, halogen free polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | Injection Molding; ISO 2577 |
Vyncolit 2940 W Novolac Phenolic Mineral and glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. USES: Multi-V pulleys and solenoid covers.Information provided by Vyncolit, a Sumitomo Bak .. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | |
Toyobo TS401 PPS, 40% Glass Fiber Reinforced Key Feature: General Purpose Grade - balanced characteristics suitable for a broad range of uses.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a spec.. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | ASTM D2566 |
BCC Products DP-11-90 Urethane Casting DP-11-90 is an unfilled, low viscosity, quick setting two component urethane system. An easy to use 1 to 1 mix ratio (Part A/Part B), DP-11-90 offers the user a 3 minute working time with parts demo.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.011 cm/cm | 0.0025 - 0.011 in/in | ASTM D955 |
Cheng Yu Plastic E2320 Flame Retardant PET, 20% Glass Fiber |
|||
Linear Mold Shrinkage | 0.0025 - 0.0040 cm/cm | 0.0025 - 0.0040 in/in | |
Bulk Molding Compounds BMC 605L Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605L molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
Bulk Molding Compounds BMC 902 Thermoset Polyester, Soft Flow Encapsulation Grade BMC 902 is a medium strength, high flow molding compound that meets Ford Specification ESFM3D114- A. BMC 902 has excellent electrical properties and creep resistance. It can be pigmented in a wide r.. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | |
BCC Products BC 8690E Polyurethane Elastomer BC 8690E is a two-component urethane elastomer compound specifically designed for casting applications. This product is a safe, easy-to-handle, room temperature mixing and curing system that contain.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0040 cm/cm | 0.0025 - 0.0040 in/in | |
Bulk Molding Compounds BMC 2274 Mineral Filled, Glass Reinforced Polyester BMC 2274 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression transfer and stuffer injection molding. It is a general-purpose material with medium.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYabs F20 GF17 ABS, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0025 - 0.0035 cm/cm | 0.0025 - 0.0035 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH GF5035 PD2 VT Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled/Heat Resistant Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | |
E-Polymers SEPAZ® LB40 PA6 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | LATI |
LATI LASTIROL TR G/10-V1 10% Glass Fiber Reinforced Polystyrene (PS) (UL94 V-1)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | ASTM D955 |
Sumitomo Bakelite North America FM 4005 Fiberglass Reinforced Phenolic Novolac FM 4005 is a fiberglass reinforced phenolic novolac molding compound, with excellent dimensional stability and good strength at elevated temperatures. This material is compliant with the specificat.. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | ASTM D955 |
Oxford Polymers 20GF 20% Glass Fiber Filled Polycarbonate for Injection Molding 20% Glass Fiber Filled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers. |