Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0015 cm/cm | 0.0015 in/in | ASTM D955 |
RheTech Products GC40P100-01 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Consumer goodsBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0015 cm/cm | 0.0015 in/in | ASTM D955 |
RheTech Products HP514-489 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 101E Lite Oak Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0030 cm/cm | 0.0015 - 0.0030 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 1200-30 Polyester SMC Premi-Glas® 1200-30 is a fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck and Marine body panels and interior structural components where smooth flat surfac.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0020 cm/cm | 0.0015 - 0.0020 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2143-24 CR-SX Fiberglass Reinforced Thick Molding Compound Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2205-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 3200-25 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-25 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Linear Mold Shrinkage | 0.0015 cm/cm | 0.0015 in/in | Positive Mold; ASTM D955 |
Resinoid 7051 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2103-10 CRSX Polyester BMC Premi-Glas® 2103-10 CR-SX is a 10% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0020 cm/cm | 0.0015 - 0.0020 in/in | ASTM D955 |
PolyOne Lubri-Tech™ PI-30CF/15T Polyetherimide (PEI), Carbon Fiber Reinforced, PTFE Lubricated
(discontinued Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | ISO 294-4 |
Solvay Specialty Polymers Ixef® 2011 Polyarylamide (PARA), 42% Mineral Filler
(discontinued **) Ixef 2011 is a general purpose, 42% mineral reinforcedpolyarylamide which exhibits high strength and stiffness, low warpage, and outstanding surface gloss.- Black: Ixef 2011/9000- Custom ColorableFe.. |
|||
Linear Mold Shrinkage | 0.0015 cm/cm | 0.0015 in/in | ISO 2577 |
Premix Premi-Glas® 2200-22 Fiberglass Reinforced SMC
(discontinued **) Description: Premi-Glas® 2200-22 is a fiberglass reinforced thermoset Sheet Molding Compound similar to the Premi-Glas® 2200-22 CR-SX product. Unlike the -CR-SX version, this product carries no UL.. |
|||
Linear Mold Shrinkage | 0.0015 cm/cm | 0.0015 in/in | ISO 2577 |
Menzolit Menzolit® BMC 0160 Unsaturated Polyester UP BMC 0160 is a general purpose BMC for electrical applications. Typical applications are lamp housings, canopies, covers and similar components.Information Provided by Menzolit |
|||
Linear Mold Shrinkage | 0.0015 cm/cm | 0.0015 in/in | ISO 2577 |
Menzolit Menzolit® BMC 0180 Unsaturated Polyester UP BMC 0180 is a general purpose BMC for electrical applications. Product according to type 803 DIN 16911. The glass content is on a level that combines good mould ability with good strength and stiffn.. |
|||
Linear Mold Shrinkage | 0.0015 cm/cm | 0.0015 in/in | ASTM D955 |
Sumitomo Bakelite North America RX® 643 Fiberglass Reinforced Phenolic RX 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10.Information pro.. |
|||
Linear Mold Shrinkage | 0.0015 cm/cm @Thickness 4.00 mm |
0.0015 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6600 GV 40 HWCP 40% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.0015 cm/cm @Thickness 4.00 mm |
0.0015 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6600 GV 40 HWCP 40% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Bulk Molding Compounds BMC A50-XHS Bulk molding compound Description: BMC A50XHS is a high strength bulk molding compound. It can be supplied in bulk or extruded in preweighted slugs. Due to the excellent flow and controlled reactivity, BMC A50XHS i.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Bulk Molding Compounds BMC T44 High Strength Mineral Filled Molding Compound BMC T44 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displacing .. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Bulk Molding Compounds BMC T60-6002A-WG Wear Resistant Molding Compound BMC T60-6002A-WG is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost pe.. |