Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00300 - 0.0470 cm/cm | 0.00300 - 0.0470 in/in | Average value: 0.0189 cm/cm Grade Count:112 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Linear Mold Shrinkage | 0.0260 - 0.0470 cm/cm | 0.0260 - 0.0470 in/in | Average value: 0.0357 cm/cm Grade Count:6 |
Overview of materials for Polytetrafluoroethylene (PTFE) Powder This property data is a summary of similar materials in the MatWeb database for the category "PTFE Powder". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |