Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | |
Solvay Specialty Polymers Ixef® 1023 Polyarylamide (PARA)
(discontinued **) Ixef 1023 is a 50% glass-fiber reinforced, UV stabilized polyarylamide for interior applications, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resis.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | |
Lehmann & Voss LUVOCOM® 1105-7909/GY 2 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Chemical and hydrolys.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | |
Lehmann & Voss LUVOCOM® 1106-7843 Polyether imide, with glass fiber, PTFE, lubricant modified, easy flowing Applications: Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Information provided by Lehmann & Voss & Co.KG |
|||
Linear Mold Shrinkage | 0.00050 - 0.0030 cm/cm | 0.00050 - 0.0030 in/in | |
Lehmann & Voss LUVOCOM® 1301-7294/BL PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Linear Mold Shrinkage | 0.00050 - 0.0030 cm/cm | 0.00050 - 0.0030 in/in | ASTM D955 |
Mar-Bal MB2000-5 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | ASTM D1299 |
Loxim 130 01V0 Polycarbonate, 30% Glass Filled, Flame Retardant Information provided by Loxim Industries |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | |
Lehmann & Voss LUVOCOM® 1105-7141 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Chemical and hydrolys.. |
|||
Linear Mold Shrinkage | 0.00050 - 0.0030 cm/cm | 0.00050 - 0.0030 in/in | |
Lehmann & Voss LUVOCOM® 1106-8374 Polyether imide, with carbon fiber and PTFE Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.Hig.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm @Thickness 4.00 mm |
0.0010 - 0.0030 in/in @Thickness 0.157 in |
|
Teijin Panlite® G-3430H Low Anisotropy, Glass Fiber Reinforced Polycarbonate Resin Reinforced with 30 % of special GF and improved appearance grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need good appearance and mechanical propertyPreci.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0030 cm/cm @Thickness 1.59 mm |
0.0020 - 0.0030 in/in @Thickness 0.0625 in |
ASTM D955 |
Plastics Group Polifil® GFPC-30 30% Glass-Reinforced Polycarbonate Polifil® GFPC series compounds offer a combination of improved dimensional stability and decreased flammability. The excellent balance of physical properties make the Polifil® glass-filled polycar.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | |
Polyram RamOfin PPH300G8 Polypropylene, 40% Glass Fiber 40% glass fiber reinforced polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | |
Bulk Molding Compounds BMC 1454 for Injection Molding Circuit Breakers BMC 1454 is a special low-cost material developed specifically for injection molding circuit breakers. It has considerable flame, arc and track resistance. BMC 1454 is a medium strength material wit.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | |
Bulk Molding Compounds BMC 350 Thermoset Polyester, Medium Impact BMC 350 is a cosmetic and appliance grade material with excellent heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical ap.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | |
Polyram RamOfin PPH308G8 Polypropylene, 40% Glass Fiber 40% glass fiber reinforced, heat stabilized, impact modified polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |