Linear Mold Shrinkage 0.0048 cm/cm
0.0048 in/in
ASTM D955
RheTech Products G10UP100-01 10% Glass Fiber Reinforced Polypropylene, Black, UL94-HB Rated
Applications: Consumer housingsConsumer goodsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0048 cm/cm
0.0048 in/in
STN 64 0808
Plastcom SLOVAMID 66 GF 30 FRA 5 Polyamide 66, 30% Glass Fiber, Halogen Flame Retardant
FeaturesPA 66 for injection moulding, reinforced with 30% glass fiber and halogen flame retardant. Application in electrical industry: breakers, coil forms, covers, terminals. Slightly decreased f..
Linear Mold Shrinkage 0.0048 cm/cm
0.0048 in/in
Plastcom SLOVALEN PH 49 GF 30 LW PP, 30% glass fibre, coupling agents, laser writer
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains the modifier of mechanical properties and contains modificator for laser labeling of fini..
Linear Mold Shrinkage 0.0048 cm/cm
0.0048 in/in
ASTM D955
Plenco 2308 Phenolic, Granular, Compression Molded
PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai..
Linear Mold Shrinkage 0.0048 cm/cm
0.0048 in/in
ASTM D955
Plenco 2571 Phenolic, Granular, Compression Molded
PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde..
Linear Mold Shrinkage 0.0048 cm/cm
0.0048 in/in
ASTM D955
Plenco 4485 Phenolic, Granular, Transfer Molded
PLENCO 04485 is a mineral filled phenolic molding compound offering excellent heat resistance, electrical resistance, and dimensional stability. UL recognized under component file E40654. 04485 is a..