Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00300 cm/cm
0.00300 in/in
ASTM D955
Niche Polymer PPHG30BK Homopolymer PP, 30% Glass Fiber Filled
Information provided by Niche Polymer
Linear Mold Shrinkage 0.00300 cm/cm
0.00300 in/in
ASTM D955
Niche Polymer PPHG40BK Homopolymer PP, 40% Glass Fiber Filled
Information provided by Niche Polymer
Linear Mold Shrinkage 0.00300 - 0.0157 cm/cm
0.00300 - 0.0157 in/in
Average value: 0.00849 cm/cm Grade Count:10
Overview of materials for PET + PBT Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Linear Mold Shrinkage 0.00300 - 0.00600 cm/cm
0.00300 - 0.00600 in/in
Average value: 0.00433 cm/cm Grade Count:3
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values..
Linear Mold Shrinkage 0.00300 - 0.0300 cm/cm
0.00300 - 0.0300 in/in
Average value: 0.00981 cm/cm Grade Count:32
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
Linear Mold Shrinkage 0.00300 - 0.0180 cm/cm
0.00300 - 0.0180 in/in
Average value: 0.0102 cm/cm Grade Count:24
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim..
Linear Mold Shrinkage 0.00300 - 0.00700 cm/cm
0.00300 - 0.00700 in/in
Average value: 0.00490 cm/cm Grade Count:8
Overview of materials for Polycarbonate, Aramid Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Aramid Fiber Reinforced". Each property range of values reported is minimum and maximum v..
Linear Mold Shrinkage 0.00300 - 0.00900 cm/cm
0.00300 - 0.00900 in/in
Average value: 0.00557 cm/cm Grade Count:55
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Linear Mold Shrinkage 0.00300 - 0.0250 cm/cm
0.00300 - 0.0250 in/in
Average value: 0.00889 cm/cm Grade Count:11
Overview of materials for Polypropylene, Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu..
Linear Mold Shrinkage 0.00300 - 0.00850 cm/cm
0.00300 - 0.00850 in/in
Average value: 0.00576 cm/cm Grade Count:7
Overview of materials for Phenolic, Novolac, Flock Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values o..
Linear Mold Shrinkage 0.00300 - 0.00640 cm/cm
0.00300 - 0.00640 in/in
Average value: 0.00490 cm/cm Grade Count:3
Overview of materials for Phenolic, Resole, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral Filled". Each property range of values reported is minimum and maximum values ..
Linear Mold Shrinkage 0.00300 - 0.0230 cm/cm
0.00300 - 0.0230 in/in
Average value: 0.0122 cm/cm Grade Count:38
Overview of materials for Nylon 66/6
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Linear Mold Shrinkage 0.00300 cm/cm
0.00300 in/in
cure shrinkage
Aremco Aremco-Bond™ 2315X High Temperature Epoxide Potting Compound
Improved Crack Resistance & Bond Strength. High Temperature Resistance, Thermally Conductive, Low Viscosity.
Linear Mold Shrinkage 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
ASTM D955
Bhansali Engineering Abstron KU602 ABS Heat Resistant
High ImpactInformation provided by Bhansali
Linear Mold Shrinkage 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
ASTM D955
Bhansali Engineering Abstron KU602M ABS Heat Resistant
High rigidityInformation provided by Bhansali
Linear Mold Shrinkage 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
ASTM D955
Bhansali Engineering Abstron KU650NH ABS Heat Resistant
High rigidityInformation provided by Bhansali
Linear Mold Shrinkage 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
ASTM D955
Bhansali Engineering Abstron KU650N ABS Heat Resistant
Medium/High ImpactInformation provided by Bhansali
Linear Mold Shrinkage 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
ASTM D955
Bhansali Engineering Abstron TG3MM ABS Injection Molding Grade
Medium Flow, Medium Impact, high RigidityInformation provided by Bhansali
Linear Mold Shrinkage 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
ASTM D955
Bhansali Engineering Abstron KU660 ABS Heat Resistant
Ultra Super High heat ResistantInformation provided by Bhansali
Linear Mold Shrinkage 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
ASTM D955
Bhansali Engineering Abstron KU670M ABS Heat Resistant
High rigidityInformation provided by Bhansali
Linear Mold Shrinkage 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
ASTM D955
Bhansali Engineering Abstron KU603 ABS Heat Resistant
High Impact, High RigidityInformation provided by Bhansali
Linear Mold Shrinkage 0.00300 - 0.0400 cm/cm
0.00300 - 0.0400 in/in
Average value: 0.0174 cm/cm Grade Count:39
Overview of materials for Acetal Copolymer, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu..
Linear Mold Shrinkage 0.00300 - 0.00900 cm/cm
0.00300 - 0.00900 in/in
Average value: 0.00639 cm/cm Grade Count:25
Overview of materials for Acrylic/Polycarbonate Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap..
Linear Mold Shrinkage 0.00300 - 0.00800 cm/cm
0.00300 - 0.00800 in/in
Average value: 0.00537 cm/cm Grade Count:18
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum..
Linear Mold Shrinkage 0.00300 - 0.0170 cm/cm
0.00300 - 0.0170 in/in
Average value: 0.00566 cm/cm Grade Count:40
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo..
Linear Mold Shrinkage 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
ASTM D955
Bhansali Engineering Abstron KU600N ABS Heat Resistant
High ImpactInformation provided by Bhansali
Linear Mold Shrinkage 0.00300 - 0.00600 cm/cm
0.00300 - 0.00600 in/in
Average value: 0.00450 cm/cm Grade Count:4
Overview of materials for Acrylic, Impact Modified Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified Sheet". Each property range of values reported is minimum and maximum values of..
Linear Mold Shrinkage 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
ASTM D955
Bhansali Engineering Abstron IPM3000 PMMA- ABS Alloy
Super High Gloss, High scratch resistanceInformation provided by Bhansali