Polymer Property : Linear Mold Shrinkage = 0.0027 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0027 cm/cm
0.0027 in/in
Plastcom SLOVAMID 6 GF 65 PA6, 65% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..
Linear Mold Shrinkage 0.0027 cm/cm
0.0027 in/in
ATM D955
Plenco 50045 PET, Pellet, Injection Molded, White  (discontinued **)
PLENCO 50045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is UL listed and available in white, natural, and black.Information s..
Linear Mold Shrinkage 0.0027 cm/cm
0.0027 in/in
ISO 2577
Polyram RamSter PF300G8 PBT, 40% Glass Fiber
40% Glass fiber reinforced PBT for injection molding applications.Information provided by Polyram.
Linear Mold Shrinkage 0.0027 cm/cm
0.0027 in/in
320 x 320 mm flat plaque; ISO 1183
Azdel Plus R401B02N 40% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R401B02N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m..
Linear Mold Shrinkage 0.0027 cm/cm
0.0027 in/in
ASTM D2566-69
BCC Products BC 7062-3H Epoxy Casting
BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yi..
Linear Mold Shrinkage 0.0027 cm/cm
0.0027 in/in
ASTM D955
Techmer Lehvoss Compounds Luvotech™ J-4/30 BK PA6/12  (discontinued **)
Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated.
Linear Mold Shrinkage 0.0027 cm/cm
0.0027 in/in
ASTM D955
Techmer Lehvoss Compounds Luvotech™ J-4/30/V0 BK2989 PA6/12  (discontinued **)
Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated.
Linear Mold Shrinkage 0.0027 cm/cm
0.0027 in/in
ASTM D955
Techmer Lehvoss Compounds Luvotech™ J-4/30/V0 NAT PA6/12  (discontinued **)
Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated.
Linear Mold Shrinkage 0.0027 cm/cm
0.0027 in/in
ASTM D955
Techmer Lehvoss Compounds Luvotech™ J-4/30/V0 RD6922 PA6/12  (discontinued **)
Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated.
Linear Mold Shrinkage 0.0027 cm/cm
0.0027 in/in
ASTM D955
Techmer Lehvoss Compounds Luvotech™ J-4/35 BK223 PA6/12  (discontinued **)
Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated.
Linear Mold Shrinkage 0.0027 cm/cm
0.0027 in/in
ASTM D955
Techmer Lehvoss Compounds Luvotech™ J-4/35 NAT PA6/12  (discontinued **)
Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated.
Linear Mold Shrinkage 0.0027 cm/cm
0.0027 in/in
ASTM D955
Techmer Lehvoss Compounds Luvotech™ J-4/35/HS NAT PA6/12  (discontinued **)
Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated.