Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0010 - 0.0025 cm/cm | 0.0010 - 0.0025 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2207-22 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2207-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0040 cm/cm | 0.0010 - 0.0040 in/in | |
Lehmann & Voss LUVOCOM® 1105-8205 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | |
Lehmann & Voss LUVOCOM® 1301-7953 PPS, linear, with carbon fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Linear Mold Shrinkage | 0.0010 cm/cm | 0.0010 in/in | ASTM D955 |
LG Chemical LUPOY GP-2400 General Purpose Modified PC, 40% Glass Fiber Reinforced, High Strength Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Linear Mold Shrinkage | 0.0010 cm/cm | 0.0010 in/in | ASTM D955 |
PlastxWorld CEVIAN® S1230 PC/ABS alloy Glass fiber reinforced PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 401 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | |
Polyram RamOfin PPH300G8 Polypropylene, 40% Glass Fiber 40% glass fiber reinforced polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0010 cm/cm | 0.0010 in/in | |
Eurotec® Tecomid® NB40 GR50 NL PA 6 50% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Linear Mold Shrinkage | 0.0010 cm/cm | 0.0010 in/in | |
E-Polymers TEKAPPO® JF201 Filler Reinforced Heat Resistant Dimensional Stability Flame Retardant M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | ASTM D955 |
Cheng Yu Plastic A706G1 SAN, 10% Glass Fiber |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | |
Bulk Molding Compounds BMC 1605 Low Shrink, Medium Strength BMC 1605 is an excellent low-cost HB material with low shrink and medium strength. Has excellent surface finish and gloss. Can be injection, compression or transfer molded. UL® recognized. This mat.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | |
Bulk Molding Compounds BMC 800 Thermoset Polyester, Corrosion Resistant BMC 800 compounds are UL rated 94V0/5V. These compounds exhibit excellent strength, corrosion and weather resistant properties. As with all other BMCI compounds, this Series can be supplied in logs,.. |
|||
Linear Mold Shrinkage | 0.0010 cm/cm | 0.0010 in/in | |
Abatron AboCast/AboCure 4-4/50-12 Casting Epoxy for Tooling Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.Main Advantages: FastBest rigid, chemical, and hea.. |
|||
Linear Mold Shrinkage | 0.0010 cm/cm | 0.0010 in/in | ASTM D955 |
A. Schulman ComAlloy Lubrilon® 636 Nylon 6/6, Carbon Fiber Reinforced, Proprietary Lubricant Package Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Linear Mold Shrinkage | 0.0010 cm/cm | 0.0010 in/in | Compression Molding; ISO 2577 |
Sumitomo Bakelite North America RX® 865M Novolac Phenolic Fiberglass reinforced phenolic novolac compound featuring dimensional stability, moderate impact resistance, good strength and modulus.Information provided by Vyncolit, a Sumitomo Bak Group |