Physical Properties | Metric | English | Comments |
---|---|---|---|
Slip Level | 1800 ppm | 1800 ppm | EAA; Borealis Method |
Borealis BorPURE™ RD266CF Polypropylene Random Copolymer BorPure™ RD266CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: BorPure™ RD266CF is recommended for
food packaging.. |
|||
Slip Level | 1800 ppm | 1800 ppm | EAA; Borealis Method |
Borealis RD461CF Polypropylene Random Copolymer RD461CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD461CF is recommended for food packaging, high quality stati.. |
|||
Slip Level | 1800 ppm | 1800 ppm | Erucamide |
Total PPH 3576 BB Polypropylene Homopolymer, Cast Film Polypropylene 3576 BB is recommended for use in non-oriented cast films processes. It contains an optimized level of slip and anti-block additives.3576 BB is intended for food, magazine or textile .. |
|||
Slip Level | 1800 ppm | 1800 ppm | Erucamide |
Total PPH 6088 Polypropylene Homopolymer, Cast Film Polypropylene PPH 6088 is a homopolymer polypropylene with a Melt Flow index of 9 g/10 min for the cast extrusion of film with excellent optical properties and good sterilizability.Polypropylene PPH.. |
|||
Slip Level | 1800 ppm | 1800 ppm | Erucamide |
Total PPR 6288 Random Copolymer Polypropylene, Cast Extrusion of Film Total Petrochemicals PPR 6288 is a random copolymer polypropylene with a melt flow index of 8 g/10 min for the cast extrusion of films with outstanding optical properties and easy heat weldability.P.. |