Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 3.00e+6 - 5.00e+6 g/mol | 3.00e+6 - 5.00e+6 g/mol | |
Inhance Fluoro-Seal INHANCE® UH-1045 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Molecular Weight | 3.00e+6 - 5.00e+6 g/mol | 3.00e+6 - 5.00e+6 g/mol | |
Inhance Fluoro-Seal INHANCE® UH-1080 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Molecular Weight | 3.00e+6 - 5.00e+6 g/mol | 3.00e+6 - 5.00e+6 g/mol | |
Inhance Fluoro-Seal INHANCE® UH-1250 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Molecular Weight | 3.00e+6 - 5.00e+6 g/mol | 3.00e+6 - 5.00e+6 g/mol | |
Inhance Fluoro-Seal INHANCE® UH-1500 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Molecular Weight | 3.00e+6 - 5.00e+6 g/mol | 3.00e+6 - 5.00e+6 g/mol | |
Inhance Fluoro-Seal INHANCE® UH-1700 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Molecular Weight | 3.00e+6 - 5.00e+6 g/mol | 3.00e+6 - 5.00e+6 g/mol | |
Inhance Fluoro-Seal INHANCE® UH-1900 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |