Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 430 g/mol | 430 g/mol | average |
Solvay Specialty Polymers Galden® DET PFPE Fluid Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat.. |
|||
Molecular Weight | 430 g/mol | 430 g/mol | average |
Solvay Specialty Polymers Galden® HT80 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Molecular Weight | 430 g/mol | 430 g/mol | Mn; ETM 300-83 |
ExxonMobil ESCOREZ™ 5415 Petroleum Hydrocarbon Resin Light colored cycloaliphatic hydrocarbon resin. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, natural rubber, synthetic polyisoprene, poly.. |
|||
Molecular Weight | 430 g/mol | 430 g/mol | ASTM D2502 |
ChevronTexaco ParaLux® 2401R Process Oil FeaturesPARALUX is produced using an all-hydroprocessing route which transforms the molecular structure of undesirable aromatics into highly desirable saturates. This produces a process oil with sup.. |