Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | >= 95000 g/mol | >= 95000 g/mol | Mn by GPC using polystyrene stds; TM-005 |
AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets Elast-Eon™ 2-852 is a polyurethane with a 52% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM.. |
|||
Molecular Weight | >= 95000 g/mol | >= 95000 g/mol | Mn by GPC using polystyrene stds; TM-005 |
AorTech Biomaterials Elast-Eon™ E2-860 Biomedical Polyurethane Pellets Elast-Eon™ 2-860 is a polyurethane with a 60% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM.. |
|||
Molecular Weight | >= 95000 g/mol | >= 95000 g/mol | Mn by GPC using polystyrene stds; TM-005 |
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets Elast-Eon™ 2A is a polyurethane with a 40% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DMAc... |
|||
Molecular Weight | >= 95000 g/mol | >= 95000 g/mol | Mn by GPC using polystyrene stds; TM-005 |
AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets Elast-Eon™ 2-852 is a polyurethane with a 52% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM.. |
|||
Molecular Weight | >= 95000 g/mol | >= 95000 g/mol | Mn by GPC using polystyrene stds; TM-005 |
AorTech Biomaterials Elast-Eon™ E2-860 Biomedical Polyurethane Pellets Elast-Eon™ 2-860 is a polyurethane with a 60% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM.. |
|||
Molecular Weight | >= 95000 g/mol | >= 95000 g/mol | Mn by GPC using polystyrene stds; TM-005 |
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets Elast-Eon™ 2A is a polyurethane with a 40% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DMAc... |
|||
Molecular Weight | >= 95000 g/mol | >= 95000 g/mol | Mn by GPC using polystyrene stds; TM-005 |
AorTech Biomaterials Elast-Eon™ E5-325 Biomedical Polyurethane Pellets Elast-Eon™ 5-325 is a polyurethane with a 32.5% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in .. |
|||
Molecular Weight | >= 95000 g/mol | >= 95000 g/mol | Mn by GPC using polystyrene stds; TM-005 |
AorTech Biomaterials Elast-Eon™ E5-325 Biomedical Polyurethane Pellets Elast-Eon™ 5-325 is a polyurethane with a 32.5% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in .. |
|||
Molecular Weight | 95000 g/mol | 95000 g/mol | Average value: 95000 g/mol Grade Count:4 |
Overview of materials for Silicone Polyurethane, Ether Based This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum value.. |