Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 8.0 - 15 m²/g | 8.0 - 15 m²/g | BET |
Nabaltec NABALOX® NO 102 Calcined Aluminum Oxide NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | 6.0 - 15 m²/g | 6.0 - 15 m²/g | BET |
Magyar Aluminum ALO-DF2 Alumina Alumina for Polishing |
|||
Specific Surface Area | 6.0 - 15 m²/g | 6.0 - 15 m²/g | BET |
Magyar Aluminum ALO-P90-02 Alumina Alumina for Polishing |
|||
Specific Surface Area | 6.0 - 15 m²/g | 6.0 - 15 m²/g | BET |
Magyar Aluminum ALO-P90-06 Alumina Alumina for Polishing |
|||
Specific Surface Area | 6.0 - 15 m²/g | 6.0 - 15 m²/g | BET |
Magyar Aluminum ALO-P90-20 Alumina Alumina for Polishing |
|||
Specific Surface Area | 12 - 15 m²/g | 12 - 15 m²/g | |
Imerys Alumex™ Kaolin Alumex is a Hydrated Aluminum Silicate used as a low surface area “soft†filler for Elastomeric systems.Information provided by Imerys |
|||
Specific Surface Area | 12 - 15 m²/g | 12 - 15 m²/g | |
Imerys Hydrated Aluminum Silicate KT 90A-1 Kaolin KT 90A-1 is a Hydraetd Aluminum Silicate. It is a high surface area, fine particle size clay that is well suited for use as an econoMical filler.Information provided by Imerys |
|||
Specific Surface Area | 12 - 15 m²/g | 12 - 15 m²/g | |
Imerys Kaolexâ„¢ FG Kaolin Kaolex FG is a air floated Hydrated Aluminum Silicate. Its low surface area makes it a good choice for fiberglass manufacturing.Information provided by Imerys |
|||
Specific Surface Area | 12 - 15 m²/g | 12 - 15 m²/g | |
Imerys Kaolexâ„¢ SC Kaolin Kaolex SC is an air floated Hydrated Aluminum Silicate. It is a low surface area, low viscosity, medium casting filler/extender for ceramic applications.Information provided by Imerys |
|||
Specific Surface Area | 12 - 15 m²/g | 12 - 15 m²/g | BET |
H.C. Starck Grade M11 h.p. Silicon Nitride, Si3N4 Higher purity, >99.995%Ceramic cutting toolsHeavy duty components in automotive enginesHigh performance parts for mechanical engineeringBearing components, like high precision ballsSiAlONsMetallurgy.. |
|||
Specific Surface Area | 12 - 15 m²/g | 12 - 15 m²/g | BET |
H.C. Starck Grade M11 I.o. Silicon Nitride, Si3N4 Alpha-phase > 90%, low oxygen content |
|||
Specific Surface Area | 12 - 15 m²/g | 12 - 15 m²/g | BET |
H.C. Starck Grade M11 Silicon Nitride, Si3N4 Alpha-phase > 90%, very narrow particle size distribution.Ceramic cutting toolsHeavy duty components in automotive enginesHigh performance parts for mechanical engineeringBearing components, like hi.. |
|||
Specific Surface Area | 14 - 15 m²/g | 14 - 15 m²/g | External |
St. Cloud Natural Zeolite (Clinoptilolite) Natural zeolites are microporous volcanic minerals with sieving and cation exchange properties for use in agriculture, environmental and industrial applications. Features such as a vary large inter.. |
|||
Specific Surface Area | 6.0 - 15 m²/g | 6.0 - 15 m²/g | |
Terio Corporation TZY-10 Yttria Stabilized Zirconia Information provided by TERIO Corporation. |
|||
Specific Surface Area | 6.0 - 15 m²/g | 6.0 - 15 m²/g | |
Terio Corporation TZY-8 Yttria Stabilized Zirconia Information provided by TERIO Corporation. |
|||
Specific Surface Area | 8.0 - 15 m²/g | 8.0 - 15 m²/g | |
Momentive Performance Materials PolarTherm® PT160 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic componen.. |