Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 5.0 m²/g | 5.0 m²/g | BET |
Nabaltec NABALOX® NO 635 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | 5.0 - 8.0 m²/g | 5.0 - 8.0 m²/g | BET |
Magyar Aluminum ALOLT 90DLS Aluminum Hydroxide Fine Precipitated Type |
|||
Specific Surface Area | 5.0 - 8.0 m²/g | 5.0 - 8.0 m²/g | BET |
Magyar Aluminum ALOLT 90F Aluminum Hydroxide Fine Precipitated Type |
|||
Specific Surface Area | 5.0 - 10 m²/g | 5.0 - 10 m²/g | |
MarkeTech H-2 Honeycomb Ceramic MarkeTech International special honeycomb ceramics have a uniform lattice structure, low expansion coefficient, good thermal shock resistance, higher specific surface area, low-pressure drop, and lo.. |
|||
Specific Surface Area | 5.0 - 10 m²/g | 5.0 - 10 m²/g | |
MarkeTech H-3 Honeycomb Ceramic MarkeTech International special honeycomb ceramics have a uniform lattice structure, low expansion coefficient, good thermal shock resistance, higher specific surface area, low-pressure drop, and lo.. |
|||
Specific Surface Area | 5.0 - 10 m²/g | 5.0 - 10 m²/g | |
MarkeTech H-4 Honeycomb Ceramic MarkeTech International special honeycomb ceramics have a uniform lattice structure, low expansion coefficient, good thermal shock resistance, higher specific surface area, low-pressure drop, and lo.. |
|||
Specific Surface Area | 5.0 - 10 m²/g | 5.0 - 10 m²/g | BET |
H.C. Starck Grade A Yttrium Oxide Sintering additive for Si3N4 and AlNStabilizer for zirconias (PSZ) and insulating coatings (TBC`s)Catalyst carrierYttria stabilized zirconias electrolytes for solid oxide fuel cellsLuminescent mater.. |
|||
Specific Surface Area | >= 5.0 m²/g | >= 5.0 m²/g | BET |
H.C. Starck Grade III Amorphous Boron Automotive (igniter in airbags and belt tighteners)Additive in pyrotechnic mixtures (flares, igniters, and delay compositions)Additive in solid rocket propellant fuels and explosivesPreparation of r.. |
|||
Specific Surface Area | 5.0 m²/g | 5.0 m²/g | BET |
TIMCAL TIMREX® SFG44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Specific Surface Area | 5.0 - 10 m²/g | 5.0 - 10 m²/g | |
American Elements Aluminum Nanoparticles General DescriptionAluminum (Al) Nanoparticles, nanodots or Nanopowder are black spherical high surface area metal particles. Nanoscale Aluminum Particles are typically 10-30 nanometers (nm) with sp.. |
|||
Specific Surface Area | 5.0 - 10 m²/g | 5.0 - 10 m²/g | |
American Elements Gadolinium Nanoparticles General DescriptionGadolinium (Gd) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Gadolinium Particles are typically 10 - 45 nanometers (nm) with sp.. |
|||
Specific Surface Area | 5.0 - 10 m²/g | 5.0 - 10 m²/g | |
American Elements Lanthanum Nanoparticles General DescriptionLanthanum (La) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Lanthanum Particles are typically 5 - 40 nanometers (nm) with speci.. |
|||
Specific Surface Area | 5.0 - 50 m²/g | 5.0 - 50 m²/g | |
American Elements Lithium Vanadate Nanoparticles General DescriptionLithium Vanadate or Lithium Vanadium Oxide (LiVO) Nanoparticles, nanodots or nanopowder are spinel, high surface area particles. Nanoscale Lithium Vanadate or Lithium Vanadium Oxi.. |
|||
Specific Surface Area | 5.0 - 10 m²/g | 5.0 - 10 m²/g | |
American Elements Neodymium Nanoparticles General DescriptionNeodymium (Nd) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Neodymium Particles are typically 10 - 45 nanometers (nm) with spec.. |
|||
Specific Surface Area | 5.0 - 10 m²/g | 5.0 - 10 m²/g | |
American Elements Nickel Nanoparticles General DescriptionNickel (Ni) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Nickel Particles are typically 10 - 40 nanometers (nm) with specific s.. |
|||
Specific Surface Area | 5.0 - 10 m²/g | 5.0 - 10 m²/g | |
American Elements Nickel Titanium Nanoparticles General DescriptionNickel Titanium (NiTi) Nanoparticles, nanodots or nanopowder are black spherical high surface area alloy particles. Nanoscale Nickel Titanium Particles are typically 10 - 40 nanom.. |
|||
Specific Surface Area | 5.0 - 10 m²/g | 5.0 - 10 m²/g | |
American Elements Silicon Nanoparticles General DescriptionSilicon (Si) Nanoparticles, nanodots or Nanopowder are spherical high surface area metal particles. Nanoscale Silicon Particles are typically 5-25 nanometers (nm) with specific su.. |
|||
Specific Surface Area | 5.0 - 10 m²/g | 5.0 - 10 m²/g | |
American Elements Strontium Carbonate Nanoparticles General DescriptionStrontium Carbonate (SrCO3) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Strontium Carbonate Particles are typically 5 - 40 nan.. |
|||
Specific Surface Area | 5.0 - 10 m²/g | 5.0 - 10 m²/g | |
American Elements Tin Oxide Nanopowder General DescriptionTin Oxide ( SnO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Tin Oxide Parti.. |
|||
Specific Surface Area | 5.0 - 10 m²/g | 5.0 - 10 m²/g | |
American Elements Tungsten Oxide Nanopowder General DescriptionTungsten Oxide ( WO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Tin Oxide P.. |
|||
Specific Surface Area | 5.0 - 10 m²/g | 5.0 - 10 m²/g | |
American Elements Yttrium Nanoparticles General DescriptionYttrium (Y) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Yttrium Particles are typically 5 - 45 nanometers (nm) with specific s.. |
|||
Specific Surface Area | 5.0 - 10 m²/g | 5.0 - 10 m²/g | |
American Elements Zirconium Nanoparticles General DescriptionZirconium (Zr) Nanoparticles, nanodots or Nanopowder are black spherical high surface area metal particles. Nanoscale Zirconium Particles are typically 10-40 nanometers (nm) with .. |
|||
Specific Surface Area | 5.0 - 10 m²/g | 5.0 - 10 m²/g | |
American Elements Calcium Oxide Nanopowder General DescriptionCalcium Oxide ( CaO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Na.. |
|||
Specific Surface Area | 5.0 - 10 m²/g | 5.0 - 10 m²/g | |
American Elements Cerium Nanoparticles General DescriptionCerium (Ce) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Cerium Particles are typically 5 - 40 nanometers (nm) with specific su.. |
|||
Specific Surface Area | 5.0 - 10 m²/g | 5.0 - 10 m²/g | |
American Elements Copper Nanoparticles General DescriptionCopper (Cu) Nanoparticles, nanodots or Nanopowder are black brown spherical high surface area metal particles. Nanoscale Copper Particles are typically 10-30 nanometers (nm) with .. |
|||
Specific Surface Area | 5.0 m²/g | 5.0 m²/g | |
BASF Sicotan® Yellow K 2011 Color Additive Chemical Structure: Cr/Sb/Ti-oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA, PETP, CA/CAB and UPRecommendations for food applications: B.. |
|||
Specific Surface Area | 5.0 m²/g | 5.0 m²/g | |
BASF Sicotan® Yellow L 1910 Color Additive Description: Mixed-phase pigment with maximum fastness properties. Suitable for all coatings systemsChemical Structure: Cr/Sb/Ti-OxideSuitable for: Baking System, Waterborn systems, Acrylic-isocyana.. |
|||
Specific Surface Area | 5.0 m²/g | 5.0 m²/g | |
3M W-210 Ceramic Microspheres 3M™ White Ceramic Microspheres are unique, semi-transparent, white-colored, fine particle size, high-strength microspheres. These products are typically used to reduce VOC levels; increase filler l.. |