Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 70 - 80 m²/g | 70 - 80 m²/g | BET Analysis |
Gwent Electronic Materials P2121112P11 Oxygen Plasma Modified Multiwalled Carbon Nanotubes Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Specific Surface Area | 70 - 80 m²/g | 70 - 80 m²/g | BET Analysis |
Gwent Electronic Materials P2121112P12 Acid Vapor Plasma Modified Single and Double Walled Carbon Nanotubes Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Specific Surface Area | 70 - 80 m²/g | 70 - 80 m²/g | BET Analysis |
Gwent Electronic Materials P2121112P13 Argon Plasma Modified Single and Double Walled Carbon Nanotubes Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Specific Surface Area | 70 - 80 m²/g | 70 - 80 m²/g | BET Analysis |
Gwent Electronic Materials P2121112P14 Nitrogen Plasma Modified Single and Double Walled Carbon Nanotubes Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Specific Surface Area | 70 - 80 m²/g | 70 - 80 m²/g | BET Analysis |
Gwent Electronic Materials P2121112P15 Ammonia Plasma Modified Single and Double Walled Carbon Nanotubes Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Specific Surface Area | 70 - 80 m²/g | 70 - 80 m²/g | BET Analysis |
Gwent Electronic Materials P2121112P16 Oxygen Plasma Modified Single and Double Walled Carbon Nanotubes Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Specific Surface Area | 70 - 80 m²/g | 70 - 80 m²/g | BET Analysis |
Gwent Electronic Materials P2121112P18 Nitrogen Plasma Modified Multiwalled Carbon Nanotubes Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Specific Surface Area | 70 - 80 m²/g | 70 - 80 m²/g | BET Analysis |
Gwent Electronic Materials P2121112P19 Tetrafluoromethane Plasma modified Single and Double Walled Carbon Nanotubes Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Specific Surface Area | 70 - 80 m²/g | 70 - 80 m²/g | BET Analysis |
Gwent Electronic Materials P2121112P7 Acid Vapor Plasma Modified Multiwalled Carbon Nanotubes Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Specific Surface Area | 70 - 80 m²/g | 70 - 80 m²/g | BET Analysis |
Gwent Electronic Materials P2121112P8 Argon Plasma Modified Multiwalled Carbon Nanotubes Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Specific Surface Area | 70 - 80 m²/g | 70 - 80 m²/g | BET Analysis |
Gwent Electronic Materials P2121112P9 Tetrafluoromethane Plasma Modified Multiwalled Carbon Nanotubes Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Specific Surface Area | 70 - 80 m²/g | 70 - 80 m²/g | BET Analysis |
Gwent Electronic Materials P2121112P10 Ammonia Plasma Modified Multiwalled Carbon Nanotubes Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Specific Surface Area | 10 - 80 m²/g | 10 - 80 m²/g | |
American Elements Tin Oxide Nanopowder General DescriptionTin Oxide ( SnO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Tin Oxide Parti.. |
|||
Specific Surface Area | 10 - 80 m²/g | 10 - 80 m²/g | |
American Elements Tungsten Oxide Nanopowder General DescriptionTungsten Oxide ( WO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Tin Oxide P.. |
|||
Specific Surface Area | 30 - 80 m²/g | 30 - 80 m²/g | |
American Elements Zirconium Nanoparticles General DescriptionZirconium (Zr) Nanoparticles, nanodots or Nanopowder are black spherical high surface area metal particles. Nanoscale Zirconium Particles are typically 10-40 nanometers (nm) with .. |