Gwent Electronic Materials P2121112P15 Ammonia Plasma Modified Single and Double Walled Carbon Nanotubes

Category Carbon
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials P2121112P15 Ammonia Plasma Modified Single and Double Walled Carbon Nanotubes.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Bulk Density 0.190 g/cc
0.00686 lb/in³
EN ISO 60
Density 1.70 - 1.90 g/cc
0.0614 - 0.0686 lb/in³
theoretical
Specific Surface Area 70 - 80 m²/g
70 - 80 m²/g
BET Analysis
Component Elements Properties Metric English Comments
Carbon, C 86.44 %
86.44 %
XPS
Fluorine, F 1.22 %
1.22 %
XPS
Nitrogen, N 5.57 %
5.57 %
XPS
Oxygen, O 6.56 %
6.56 %
XPS
Silicon, Si <= 0.010 %
<= 0.010 %
XPS
Descriptive Properties Value Comments
Nanotube Length, nm 1000
SEM
Nanotube Outer Diameter, nm 1-5
SEM
Zeta Potential, mV -18.5
LDE