Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 8.0 - 12 m²/g | 8.0 - 12 m²/g | BET |
Nabaltec NABALOX® NO 113 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | 8.0 - 12 m²/g | 8.0 - 12 m²/g | BET |
Nabaltec NABALOX® NO 313 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | 8.0 - 12 m²/g | 8.0 - 12 m²/g | BET |
Nabaltec NABALOX® NO 713-40 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | 6.0 - 12 m²/g | 6.0 - 12 m²/g | BET |
Magyar Aluminum ALO-Ex325 Alumina Calcined Alumina |
|||
Specific Surface Area | 6.0 - 12 m²/g | 6.0 - 12 m²/g | BET |
Magyar Aluminum ALO-G32-2 Alumina Ground Alumina |
|||
Specific Surface Area | 8.0 - 12 m²/g | 8.0 - 12 m²/g | BET |
Magyar Aluminum ALOLT 120F Aluminum Hydroxide Fine Precipitated Type |
|||
Specific Surface Area | 6.0 - 12 m²/g | 6.0 - 12 m²/g | BET |
Magyar Aluminum ALO-P90 Alumina Alumina for Polishing |
|||
Specific Surface Area | 6.0 - 12 m²/g | 6.0 - 12 m²/g | BET |
H.C. Starck Grade B Yttrium Oxide Sintering additive for Si3N4 and ALNStabilizer for zirconias (PSZ) and insulating coatings (TBC`s)Catalyst carrierYttria stabilized zirconias electrolytes for solid oxide fuel cellsLuminescent mater.. |
|||
Specific Surface Area | 10 - 12 m²/g | 10 - 12 m²/g | High Range |
Vesta Ceramics SicoNide® P Silicon Nitride Powder General Description:SicoNide® is a silicon nitride powder with a broad particle size distribution allowing better, tighter packing when pressed. Our computer-controlled production processes guaran.. |
|||
Specific Surface Area | 10 - 12 m²/g | 10 - 12 m²/g | High Range |
Vesta Ceramics SicoNide® S S Silicon Nitride Powder General Description:SicoNide® is a silicon nitride powder with a broad particle size distribution allowing better, tighter packing when pressed. Our computer-controlled production processes guaran.. |
|||
Specific Surface Area | 7.0 - 12 m²/g | 7.0 - 12 m²/g | Nitrogen; ASTM D6556 |
Cancarb Thermax® Floform N907 Stainless Medium Carbon Black Thermal carbon black, often referred to as MT black, is unique in several ways. Along the carbon black spectrum, it has the largest particle size and among the lowest degrees of particle aggregation.. |
|||
Specific Surface Area | 7.0 - 12 m²/g | 7.0 - 12 m²/g | Nitrogen; ASTM D6556 |
Cancarb Thermax® Powder N908 Stainless Medium Carbon Black Thermal carbon black, often referred to as MT black, is unique in several ways. Along the carbon black spectrum, it has the largest particle size and among the lowest degrees of particle aggregation.. |