Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 1.2 - 1.8 m²/g | 1.2 - 1.8 m²/g | BET |
Nabaltec NABALOX® NO 615-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | 1.2 - 1.8 m²/g | 1.2 - 1.8 m²/g | BET |
Nabaltec NABALOX® NO 625-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |