Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 20 m²/g | 20 m²/g | |
Old Hickory FC-340 Tennessee Ball Clay The FC-340 clay is designed for all types of casting formulas ranging from low fire earthenware to vitreous composition. It has excellent response to deflocculation and a very good casting rate whil.. |
|||
Specific Surface Area | 20 m²/g | 20 m²/g | |
Omya HYDROCARB® HG Calcium Carbonate An ultrafine ground calcium carbonate for paper and board coating.Information supplied by Omya North America. |
|||
Specific Surface Area | 20 m²/g | 20 m²/g | Statistical thickness surface area; ASTM D 6556 |
Orion Engineered Carbons PUREX® HS 22 Carbon Black Carbon black grade for manufacture of mechanical rubber goods such as extruded profiles and sealsInformation provided by Orion Engineered Carbons. |
|||
Specific Surface Area | >= 20 m²/g | >= 20 m²/g | BET |
NanoScale NanoActive® Calcium Oxide NanoActive CaO is produced using proprietary processes to obtain high specific surface area (over 20 m²/g vs. 1-2 m²/g for standard CaO) with strong affinity towards carbon dioxide and hydrogen su.. |
|||
Specific Surface Area | 20 m²/g | 20 m²/g | |
Imerys #6 Tileâ„¢ Kaolin #6 Tile is a high plasticity kaolin. It is well known for its contribution to high unfired strength plasticity and white fired properties. Information provided by Imerys. |
|||
Specific Surface Area | 20 m²/g | 20 m²/g | |
GrafTech GRAFOIL® TG679 Expanded Natural Graphite Powder GRAFOIL® Grade TG679 is an expanded natural graphite powder with consistent purity and good lubrication properties. Typical applications include using the graphite powder as an electrically condu.. |
|||
Specific Surface Area | 20 m²/g | 20 m²/g | |
Momentive Performance Materials NX1 Boron Nitride (BN) Powder Grades NX1, NX5, NX9, and NX10. The NX line makes BN accessible to users of alternate materials, such as aluminum nitride, alumina, and fused silica, who may have previously ruled out BN.NX grades a.. |
|||
Specific Surface Area | 20 m²/g | 20 m²/g | BET |
TIMCAL C-NERGY™ KS 6L Graphite Product Characteristics:The total Fe content for our conductive carbon blacks is less than 5 ppm The total Fe content for our graphite is less than 20 ppmC-NERGY grades have very low total metallic .. |
|||
Specific Surface Area | 20 m²/g | 20 m²/g | BET |
TIMCAL TIMREX® KS15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Specific Surface Area | 20 m²/g | 20 m²/g | BET Analysis |
Goodfellow HDPlas® GNP Plasma Functionalized Graphene Nanoplatelets Graphene is a carbon based material which is inherently inert and which does not like to mix with, or bond to, other materials. Its excellent properties can only be fully realized when this fundamen.. |
|||
Specific Surface Area | 20 m²/g | 20 m²/g | ATO 40-45-0 (BET) |
Arkema Group ORGASOL® 3501 EXD Nat 1 Copolyamide 6/12 Information provided by Arkema Group |
|||
Specific Surface Area | >= 20 m²/g | >= 20 m²/g | Internal Method |
Solvay Specialty Polymers Algoflon® L100 Polytetrafluoroethylene (PTFE)
(Unverified Data**) Algoflon® L100 is a white PTFE micropowder comprising loose agglomerates of sub-micron sized particles. Algoflon® L100 is specially polymerized to obtain a powder with exceptionally high specific .. |
|||
Specific Surface Area | 20 m²/g | 20 m²/g | |
BASF Sicopal® Blue K 6310 Color Additive Chemical Structure: Co/Al-oxideApplication: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA PETP, CA/CAB and UPRecommendations for food applications: .. |