Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 30 - 60 µm | 30 - 60 µm | mesh. |
Oceanchem Group Calcium Chloride 94-95% powder Molecular Formula: CaCl2Information Provided by Oceanchem Group |
|||
Particle Size | 35 - 60 µm | 35 - 60 µm | average |
Momentive Performance Materials PolarTherm® PT110 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp.. |
|||
Particle Size | 50 - 60 µm | 50 - 60 µm | 90% |
H.C. Starck Amperit® 105.074 Agglomerated Sintered Molybdenum (Mo) |
|||
Particle Size | 50 - 60 µm | 50 - 60 µm | 90% |
H.C. Starck Amperit® 538.074 Agglomerated, Sintered Tungsten Carbide-Tungsten Boride-Cobalt (WC-WB-Co ) 60-30-10 |
|||
Particle Size | 50 - 60 µm | 50 - 60 µm | 90% |
H.C. Starck Amperit® 559.074 Agglomerated, Sintered Tungsten Carbide-Cobalt-Chromium 86-6-8 (WC-Co-Cr) |
|||
Particle Size | 52 - 60 µm | 52 - 60 µm | 90% |
H.C. Starck Amperit® 586.1 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr) |
|||
Particle Size | 40 - 60 µm | 40 - 60 µm | |
Lucite International Colacryl ® D150 Acrylic Dental Resin A range of Methyl Methacrylate polymers designed for use as standard heat-curing denture base resins.Features: Fine free-flowing bead polymers containing residual peroxide initiator; Curing cycles f.. |
|||
Particle Size | 50 - 60 µm | 50 - 60 µm | |
Lucite International Colacryl ® D80FC Acrylic Dental Resin Methyl Methacrylate polymers and copolymers designed for use as fast heat curing denture base resins.Colacryl denture base resins feature fast polymerisation and a wide choice of process properties... |
|||
Particle Size | 50 - 60 µm | 50 - 60 µm | |
Lucite International Colacryl ® TS2050 Acrylic Resin Lucite® Colacryl® TS2050 is a hard, methyl methacrylate based, acrylic resin with an especially tight particle size distribution, leading to extremely good performance in glass separation appl.. |
|||
Particle Size | 50 - 60 µm | 50 - 60 µm | 90% |
H.C. Starck Amperit® 140.3 Tungsten (W) HS Number: 81011000 |
|||
Particle Size | 50 - 60 µm | 50 - 60 µm | 90% |
H.C. Starck Amperit® 146.3 Chromium (Cr) HS Number: 81122031 |
|||
Particle Size | 20 - 60 µm | 20 - 60 µm | |
DayGlo ZQ Pigments ZQ-11 Aurora Pink DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Particle Size | 20 - 60 µm | 20 - 60 µm | |
DayGlo ZQ Pigments ZQ-12 Neon Red DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Particle Size | 20 - 60 µm | 20 - 60 µm | |
DayGlo ZQ Pigments ZQ-13 Rocket Red DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Particle Size | 20 - 60 µm | 20 - 60 µm | |
DayGlo ZQ Pigments ZQ-14 Fire Orange DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Particle Size | 20 - 60 µm | 20 - 60 µm | |
DayGlo ZQ Pigments ZQ-15 Blaze Orange DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Particle Size | 20 - 60 µm | 20 - 60 µm | |
DayGlo ZQ Pigments ZQ-16 Arc Yellow DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Particle Size | 20 - 60 µm | 20 - 60 µm | |
DayGlo ZQ Pigments ZQ-17 Saturn Yellow DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Particle Size | 20 - 60 µm | 20 - 60 µm | |
DayGlo ZQ Pigments ZQ-18 Signal Green DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Particle Size | 20 - 60 µm | 20 - 60 µm | |
DayGlo ZQ Pigments ZQ-19 Horizon Blue DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Particle Size | 20 - 60 µm | 20 - 60 µm | |
DayGlo ZQ Pigments ZQ-21 Corona Magenta DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |