Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 20.0 - 50.0 µm | 20.0 - 50.0 µm | Average value: 32.0 µm Grade Count:5 |
Overview of materials for Epoxy Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Particle Size | 2.00 - 50.0 µm | 2.00 - 50.0 µm | Average value: 30.4 µm Grade Count:43 |
Overview of materials for Epoxy, Electrically Conductive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of.. |
|||
Particle Size | 5.00 - 50.0 µm | 5.00 - 50.0 µm | Average value: 27.5 µm Grade Count:3 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |