Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 22 - 26 µm | 22 - 26 µm | 10% |
H.C. Starck Amperit® 519.088 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO) |
|||
Particle Size | 22 - 26 µm | 22 - 26 µm | 10% |
H.C. Starck Amperit® 526.088 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17 |
|||
Particle Size | 22 - 26 µm | 22 - 26 µm | 10% |
H.C. Starck Amperit® 527.088 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17 |
|||
Particle Size | 22 - 26 µm | 22 - 26 µm | 10% |
H.C. Starck Amperit® 588.088 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) 53/20 µm |
|||
Particle Size | 22 - 26 µm | 22 - 26 µm | 10% |
H.C. Starck Amperit® 547.074 Tungsten Carbide-Nickel 88-12 (WC-Ni) |
|||
Particle Size | 24 - 26 µm | 24 - 26 µm | D50 |
Sinotek Materials ZSG-25 Spherical Graphite Also called "Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, a series of shaping, classification.. |