Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 7.0 - 14 µm | 7.0 - 14 µm | average |
Malvern Minerals Novacite® 1250 Untreated Lamellar Quartz Filler/Extender Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
Particle Size | 7.0 - 14 µm | 7.0 - 14 µm | average |
Malvern Minerals Novakup® 1250 Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Particle Size | 8.0 - 14 µm | 8.0 - 14 µm | average |
Momentive Performance Materials PolarTherm® PT120 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp.. |
|||
Particle Size | 1.6 - 14 µm | 1.6 - 14 µm | d10 |
Indium Corp. In(OH)3 Crystalline Indium Hydroxide Indium Acetate is a white powder. Crystalline Form: Primary particles range from 1 to 5 microns in size. They are cubic in shape and form agglomerates up to approximately 35 microns.PropertiesChe.. |
|||
Particle Size | 10 - 14 µm | 10 - 14 µm | 10% |
H.C. Starck Amperit® 553.065 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr) |
|||
Particle Size | 10 - 14 µm | 10 - 14 µm | d90, Guaranteed |
TIMCAL TIMREX® PP 10 Natural Flake Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | 8.0 - 14 µm | 8.0 - 14 µm | average |
Momentive Performance Materials PolarTherm® PT140 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic componen.. |