Indium Corp. In(OH)3 Crystalline Indium Hydroxide

Category Ceramic , Oxide
Manufacturer Indium Corporation of America
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. In(OH)3 Crystalline Indium Hydroxide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Indium Acetate is a white powder. Crystalline Form: Primary particles range from 1 to 5 microns in size. They are cubic in shape and form agglomerates up to approximately 35 microns.PropertiesChemical Formula: In(OH)3Purity Grade Available: 4N (99.99%), 5N (99.999%)Solubility: Soluble in mineral acids; insoluble in water.UsesChemical synthesis.Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Particle Size 1.6 - 14 µm
1.6 - 14 µm
d10
8.9 - 28 µm
8.9 - 28 µm
d50
15 - 46 µm
15 - 46 µm
d90
Specific Surface Area 5.7 m²/g
5.7 m²/g
BET
Molecular Weight 165.94 g/mol
165.94 g/mol
Component Elements Properties Metric English Comments
Indium, In 67.9 - 69.7 %
67.9 - 69.7 %
69.24 %
69.24 %
Theoretical