Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 110.2 Agglomerated Sintered (Mo-Mo2C)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 515.074 Sintered Tungsten Carbide - Cobalt (WC-Co) 88-12
HS Number: 28499030 |
Particle Size |
<= 88 µm |
<= 88 µm |
100% less than |
H.C. Starck Amperit® 515.1 Sintered Tungsten Carbide - Cobalt (WC-Co) 88-12
HS Number: 28499030 |
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 519.074 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 526.062 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 527.074 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 538.074 Agglomerated, Sintered Tungsten Carbide-Tungsten Boride-Cobalt (WC-WB-Co ) 60-30-10
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 539.054 Agglomerated, Sintered Tungsten Carbide-Tungsten Boride-Cobalt-Chromium (WC-WB-Co-Cr) 60-30-5-5
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 554.074 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 559.074 Agglomerated, Sintered Tungsten Carbide-Cobalt-Chromium 86-6-8 (WC-Co-Cr)
|
Particle Size |
88 µm |
88 µm |
100% less than (WC-Co 83-17) |
H.C. Starck Amperit® 560.062 Tungsten Carbide-Cobalt(83-17)-Nickel-SF RC 60 50-50 (Wc-Co / NiSF RC 60)
Composition is of NiSF RC 60 only |
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 582.072 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr)
|
Particle Size |
88 µm |
88 µm |
100% less than, Cr3C2 |
H.C. Starck Amperit® 585.3 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr)
Composition is of Cr3C2 only |
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 586.054 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 588.074 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) 45/15 µm
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 703.1 Chromium Oxide (Cr2O3) 99.5%
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 705.1 Fused Chromium Oxide 96.0 % (Cr2O3)
|
Particle Size |
88 µm |
88 µm |
100% |
H.C. Starck Amperit® 712.074 Chromium Oxide-Titanium Oxide 75-25 (Cr2O3-TiO2)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 716.054 Chromium Oxide-Titanium Oxide-Silicon Oxide 92-3-5 (Cr2O3-TiO2-SiO2)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 716.066 Chromium Oxide-Titanium Oxide-Silicon Oxide 92-3-5 (Cr2O3-TiO2-SiO2)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 740.3 Aluminum Oxide (Al2O3)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 825.1 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 553.074 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 558.074 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 599.074 Agglomerated Sintered Molybdenum Carbide (Cr2O3)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 704.3 Chromium Oxide (Cr2O3) 99.5%
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 740.1 Aluminum Oxide (Al2O3)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 745.1 Aluminum Oxide-Titanium Oxide 60-40 (Al2O3-TiO2)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 547.074 Tungsten Carbide-Nickel 88-12 (WC-Ni)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 551.074 Tungsten Carbide - Chromium Carbide - Nickel 70-20-7 (W-CrC-Ni)
|